| Electronic structure and magnetism of clusters Nin(n=2-6) |
| DONG Jianmin; LI Hua; ZHANG Changwen; PAN Fengchun; WANG Yongjuan; ZHEN Peng |
| School of Physics and Microelectronics; Shandong University; Jinan 250100 |
|
Cite this article:
DONG Jianmin; LI Hua; ZHANG Changwen; PAN Fengchun; WANG Yongjuan; ZHEN Peng. Electronic structure and magnetism of clusters Nin(n=2-6). Acta Metall Sin, 2005, 41(3): 242-244 .
|
|
|
Abstract The electronic structure and magnetism of clusters Nin(n=2-6)
have been studied by spin-polarized MS-Xα method. The results show
that the effect of the cluster symmetry on its atomic magnetic moment and
electronic density of states is very notable. Ni6 cluster is an
octahedron belonging to Oh point group. Its 3Eg orbital
presents strong negative exchange coupling and has a trend of
antiferromagnetic couplings. Ni5 cluster is of three-side pyramidal
structure belonging to point group C3v.
The magnetic moment direction
of Ni atom lying on vertex of the pyramid is antiparallel to the moment
direction of the Ni atoms lying on underside of the pyramid, which present
the characteristic of ferrimagnetic couplings. Compared with metal nickel,
the magnetic moments of some clusters are enhanced and some are weakened.
The abnormal phenomenon of surface magnetism of ferromagnetic superfine
particles can be well explained using this result.
|
|
Received: 21 June 2004
|
|
|
[1] Sato M, Hirakawa K. J Phys Soc Jpn, 1975; 39: 1467 [2] Kaiser R, Miskolczy G J. J Appl Phys, 1970; 41: 1064 [3] Liebermann L, Clinton J. Phys Rev Lett, 1970; 25: 232 [4] Fulde P, Luther A, Watson R E. Phys Rev, 1973; 8B: 440 [5] Hu W J, Mei L M, Li H. Solid State Commn, 1996; 100: 129 [6] Li J Q. Xa Method in Quantum Chemistry and Its Application, Hefei: Anhui Science and Technology Press, 1983: 108 (李俊清.量子化学中的Xa方法及其应用.合肥:安徽科学技 术出版社, 1983:108) [7] Reuser F A, Khanna S N. Chem Phys Lett, 1995; 234: 77 [8] Pastor G M, Dorantes-Davila J. Phys Rev, 1989; 40B: 7642 [9] Apsel S E, Emmert J W. Phys Rev Lett, 1996; 76: 1441 |