| STUDY OF AGING BEHAVIOR OF Cu-Nb CONTAINING STEELS BY CREEP METHOD |
| WANG Xuemin; SHANG Chengjia; YANG Shanwu; LI Chuang; HE Xinlai; ZHOU Guifeng |
| Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
WANG Xuemin; SHANG Chengjia; YANG Shanwu; LI Chuang; HE Xinlai; ZHOU Guifeng. STUDY OF AGING BEHAVIOR OF Cu-Nb CONTAINING STEELS BY CREEP METHOD. Acta Metall Sin, 2005, 41(12): 1256-1260 .
|
|
|
Abstract A creep test was conducted on a Gleeble-1500 thermal simulator for
monitoring the aging procedure of Cu-Nb ultra-low carbon steels
with different contents of copper. The result indicated that during
creep testing the occurrence of precipitation could make a plateau
on the creep curve. The left- and right-hand ending points of the
plateau can be defined as the precipitation start (Ps) and
finish (Pf) times, respectively. The Pf is in
coincidence with the peak time (tp) from hardness curve.
The precipitation-time-temperature (PTT) diagrams of two steels were obtained.
|
|
Received: 16 March 2005
|
|
|
[1] Krishnadev M R. In: Michael K ed., Proc Int Conf on Technology and Applications of HSLA Steels. Metals Park, Ohio: ASM, 1984: 129 [2] Mikalac S J, Vassilaros M G. In: Deardo A J ed., Proc Int Conf on Processing, Microstructure and Properties of Microalloyed and Other Modern High Strength Low Alloy Steels. Warrendale, PA: Iron and Steel Society, 1991: 331 [3] Hwang Q C, Lee S, Yoo J Y. Mater Sci Eng, 1998; A252: 256 [4] Wang X M, He X L, Shang C J, Yang S W, Wu H B. ISIJ Int, 2002; 42: 1553 [5] Shang C J, Wang X M, He X L., Yang S W, Yuan Y. J Univ Sci Technol Beijing, 2001; 8: 224 [6] Krishnadev M R, Galibois A. Metall Trans, 1975; 6: 222 [7] Sano N, Maehara Y. J Jpn Inst Met, 1996; 60: 261 (佐野 直幸,前原 泰裕.日本金属学会志, 1996;60:261) [8] Morita M, Sato K, Hosoya Y. ISIJ Int, 1994; 34: 92 [9] Wang X M, Zhou G F, Yang S W, He X L. Acta Metall Sin, 2000; 36: 113 (王学敏,周挂峰,杨善武,贺信莱.金属学报,2000;36:113) [10] Sun W P, Liu W J, Jonas J J. Metall Trans, 1989; 20A: 2707 [11] Kouichi M, Hideaki K, Takashi W. ISIJ Int, 1990; 30: 817 [12] Wada H, Houbaert Y, Penning J, Dilewijns J. ATB Metall, 1983; 23: 31; |