Abstract In Gasar process, the metal-gas binary system for non-compound forming,
is solidified to fabricate regular porous materials
through oriented growth. The characteristics of phase diagram of
this kind of system and the principle for calculating
the phase diagram were analyzed. The
Cu--H binary phase diagram is calculated upon the above principle.
[1] Shapovalov V I. US Pat, No. 5, 181, 549. January 26, 1993 [2] Walukas D M. GASAR Materials: A Novel Approach inthe Fabrication of Porous Materials. DMK TEK INC.,Ann Arbor, MI, 1992-1 [3] Shapovalov V I. MRS Bull, 1994; 19(4): 24 [4] http://www.mrs.org/meetings/spring98/progbook/ProgramBookR.htmlhttp://www.mrs.org/meetings/spring94/progbook/ProgramBookR.html [5] Zheng Y, Sridhar S, Russell K C. Mater Res Soc SympProc, 1995; 371. 365 [6] Yu Z. MSC Thesis, USA: MIT, 1995; 1:46 [7] Yu J Q, Yi W Z, Chen B D, Chen H J. Collective Draw-ings of Binary Alloy State Diagram. Shanghai: ShanghaiScience and Technology Press, 1987: 6(虞觉奇,易文质,陈邦迪,陈宏鉴.二元合金状态图集 上海:上海科学技术出版社, 1987:6) [8] Smithells C J. Metals Reference Book (Fifth Edition).London: Butterworth & Co., Ltd., 1976: 231 [9] Vol A E.Handbook of Binary Metallic Systems. Jerusalem:Israel Program for Scientific Translations, 1967; 2: 290 [10] Sridhar S. MSC Thesis, Sweden: Royal Institute of Tech-nology, 1994: 73 [11] Shapovalov V I, Semik A P, Timchenko A G. Metallurgy, 1993; (3) 25j
YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.