| Homogenous Flow Model for Gas Driven Circulating Flow in RH Refining System |
| LI Baokuan; HUO Huifang; LUAN Yejun QI Fengsheng |
| School of Materials and Metallurgy; Northeastern University; Shenyang 110004 |
|
Cite this article:
LI Baokuan; HUO Huifang; LUAN Yejun QI Fengsheng. Homogenous Flow Model for Gas Driven Circulating Flow in RH Refining System. Acta Metall Sin, 2005, 41(1): 60-.
|
|
|
Abstract A new revised homogenous model is proposed to solve the problem
about two phase flow in side blown reactor, in which the gas
horizontal slip velocity is introduced in the gas
conservation equation only in the injection zone, so as to
make gas into bulk melt. The computed results show that the
revised model can solve side blown problem reasonably and
the computed gas distribution agrees very well
with the experimental result.
|
|
Received: 07 January 2004
|
|
|
[1] Wei J H, Yu N W. Steelmaking Conf Proc, 2002; 85: 687 [2] Murai T, Matsuno H, Sakurai E, Kawashima H. TetsuHagane, 1998; 84: 13 [3] Szatkowski M, Tsai M C. Trans ISS, 1991; I & SM: 65 [4] Li B K, Tsukihashi F. ISIJ Int, 2000; 40: 1203 [5] Zhu M Y, Sha J, Huang Z Z. Acta Metall Sin, 2000; 36:1175(朱苗勇,沙骏,黄宗泽.金属学报, 2000;36:1175) [6] Liu Z X, Chen Y S, He Y D, Cang D Q. J Baotou InsIron Steel, 2001; 20: 19(刘中兴,陈义胜,贺友多,苍大强.包头钢铁学院学报,2001;20:19) [7] Li B K, Okane T, Umeda T. Metall Mater Trans, 2000;31B: 1491 [8] Turkoglu H, Farouk B. Steelmaking Conf Proc, 1990; 80:377 [9] Launder B E, Spalding D B. Comput Methods Appl MechEng, 1974; 3: 269 [10] Soo S L. Fluid Dynamics of Multiphase System, Waltham,MA: Blaisdell Publishing Co., 1967: 3 [11] Castillejos A H, Brimacombe J K. Metall Trans, 1987;18B: 649 [12] Luan Y J, Li G H, Huo H F, Li B K. J Anhui Univ Tech-nol, 2003; 20: 18(栾叶君,李国辉,霍慧芳,李宝宽.安徽工业大学学报,2003;20:18)I |