| Microstructure and Superplastic Deformation Behavior of NiAl-15Cr Alloy |
| GUO Jianting; ZHANG Guangye; ZHOU Jian |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
GUO Jianting; ZHANG Guangye; ZHOU Jian. Microstructure and Superplastic Deformation Behavior of NiAl-15Cr Alloy. Acta Metall Sin, 2004, 40(5): 494-498 .
|
|
|
Abstract The microstructure and deformation behavior of high temperature tension of a
directionally solidified (DS) NiAl-15Cr alloy have been investigated. The results reveal that
the microstructure consists of dendritic β-NiAl phase,
interdendritic γ/γ' phase and
transient layer γ' phase.
The alloy shows superplastic behavior when it is deformed under
the conditions of temperature range of 1123--1373 K and initial
strain rate range of 1.67×10 -4--1.67×10 -2
s-1. The maximum elongation of 280% with m=0.22 is obtained at
1323 K and an initial strain rate of 8.35×10
-3 s-1.
The superplastic mechanism for the alloy
is also discussed by the observation of the
microstructures evolution during the
superplastic deformation process.
|
|
Received: 16 May 2003
|
|
|
[1] Sherby O D, Wadsworth J. Prog Mater Sci, 1989; 33:169 [2] Takasugi T, Rikukawa S, Hanada S T. Scr Metall Mater, 1991; 25:889 [3] Kirn M S, Hanada S, Wantanade S. Mater Trans JIM, 1989; 30(1) : 77 [4] Kim W Y, Hanada S, Sakai T. Acta Matrer, 1999; 46: 3593 [5] Chouhury A, Mukurjee A K, Sikka V K. Mater Sci, 1990; 25:3142 [6] Li D Q, Shan A D, Li Y, Lin D L. Scr Metall Mater; 1995; 33:681 [7] Lin D L, Li D Q, Liu Y. Intermetallics, 1998; 6:243 [8] Dutta A, Banerjee D. Scr Metall Mater, 1990; 24:1319 [9] Imayer R M, Kaibyshe O A, Salishcher G A. Acta Metal Mater, 1992; 40:581 [10] Yang H S, Jin P, Muhkerjee A K. Mater Sci Eng, 1992; 153:457 [11] Wang B, Jia T C, Zou D X. Mater Sci Eng, 1992; A152: 317 [12] Kim H Y, Hong S H. Scr Mater, 1998; 38:1517 [13] Du X H, Guo J T, Zhou B D. Scr Mater, 2001; 45:89 [14] Zhou W L, Guo J T, Chen R S, Li G S, Zhou J Y. Mater Lett, 2001; 47:30 [15] Zhou W L, Guo J T, Chen R S, Zhou J Y. Mater Lett, 2001; 51:342 [16] Du X H, Guo J T, Zhou B D. Mater Lett, 2002; 52:442 [17] Chen R S, Guo J T, Yin W M, Zhou J Y. Scr Mater, 1999; 40:219 [18] Noebe R D, Cullers C I.J Mater Res, 1992; 7:604 [19] Uan J Y, Chen L H, Liu T S. Metall Mater Trans, 1997; 28A: 401 [20] Qi Y H, Guo J T, Cui C Y. Chin J Nonferrous Met, 2002; 12:169(齐义辉,郭建亭,崔传勇.中国有色金属学报,2002;12:169) |