EFFECT OF MOLYBDENUM ON DELAYED FRACTURE BEHAVIOR OF HIGH STRENGTH STEEL
HUI Weijun; DONG Han; WENG Yuqing; SHI Jie; ZHANG Xiaozhong
Institute of Structural Materials; Central Iron & Steel Research Institute; Beijing 100081
Cite this article:
HUI Weijun; DONG Han; WENG Yuqing; SHI Jie; ZHANG Xiaozhong. EFFECT OF MOLYBDENUM ON DELAYED FRACTURE BEHAVIOR OF HIGH STRENGTH STEEL. Acta Metall Sin, 2004, 40(12): 1274-1280 .
Abstract Four heats of V and Nb microalloyed 40Cr steel containing 0 to 1.54% Mo
were used to study the effect of Mo on delayed fracture resistance. The
results of both notched tensile sustained load test and stress corrosion
cracking test show that the delayed fracture resistance increases with
increasing Mo content. Maximum delayed fracture resistance is obtained
at a Mo concentration of about 1.15%. The result of EDS
(energy dispersive spectroscopy) analysis shows
that Mo tends to segregate in the grain boundary in a scale of no more
than a few nanometers. EELS (electron energy loss spectra) measurement
indicates that the segregation
of Mo in grain boundary tends to increase the strength of grain boundary.
The pronounced effect of Mo in raising the tempering resistance and the
ability to strengthen prior austenite grain boundary are the main reasons
for the beneficial effect of Mo on delayed fracture resistance. Hydrogen
trapping effect caused by fine Mo2C precipitation could also improve
the delayed fracture resistance. It is also confirmed that the tested
steels could have a much higher delayed fracture resistance when the
secondary hardening carbides of V and Mo are in the condition of slight
over-raging.
[1] Archer R S, Briggs J Z, Loeb C M Jr. MolybdenumSteels, Iron and Alloys. New York: Climax Molybdenum Co., 1970:1 [2] Honeycombe S R, Bhadeshia H K D H. SteelsMicro structure and Properties. 2nd ed., London: Edward Arnold, 1995: 182 [3] Dumoulin P, Guttmann M, Foucault M, Palmier M, Wayman M, Biscondi M. Met Sci, 1980: 14(1):1 [4] Grobner P J, Sponseller D L, Diesburg. Corrosion, 1979: 35(6): 240 [5] Craig B D, Krauss G. Metall Trans, 1980: 11A:1799 [6] Craig B D. Metall Trans, 1982: 13A: 1099 [7] Charbonnier J C, Margot-Marette H, Brass A M, Aucouturier M. Metall Trans, 1985:16A: 935 [8] Asahi H, Sogo Y, Ueno M, Higashiyama H. Metall Trans, 1988: 19A: 2171 [9] Xiang C Y. Alloyed Structural Steels. Beijing: Metallurgical Industry Press, 1999: 132, 335 (项程云.合金结构钢.北京:冶金工业出版社,1999:132, 335) [10] Hui W J, Dong H, Weng Y Q. Iron Steel, 2001: 36(3): 69 (惠卫军,董瀚,翁字庆.钢铁,2001:36(3):69) [11] Chu W Y. Hydrogen Damage and Delayed Failure. Beijing: Metallurgical Industry Press, 1988: 472 (褚武扬.氢损伤和滞后断裂.北京:冶金工业出版社,1988: 472) [12] Weng Y Q, et al. Ultrafine Grained Steels-The Theory of Microstructure Refinement and Controlling Technology for Steels. Beijing: Metallurgical Industry Press, 2003: 967 (翁宇庆等.超细晶钢--钢的组织细化理论与控制技术.北 京:冶金工业出版社,2003:967) [13] Hui W J. PhD Thesis, Central Iron & Steel Research Institute, Beijing, 2003 (惠卫军.钢铁研究总院博士学位论文,北京,2003) [14] Li G F, Wu R G, Lei T C. Metall Trans, 1992: 23A: 2879 [15] Hui W J, Dong H, Weng Y Q. J Iron Steel Res Int, 2003:10(4): 75 [16] Llewellyn D T. Ironmaking Steelmaking, 1996: 23: 397 [17] Gojic M, Kosec L. ISIJ Int, 1997: 37: 412 [18] Zhong P, Gu B Z, Jin J J, Wang H T. J Aeronaut Mater,1995: 15(4): 41 (钟平,古宝珠,金建军,王洪涛,航空材料学报,1995:15(4): 41) [19] Muller D A, Batson P E, Subramanian S, Sass S L, Silcox J. J Phys Rev Lett, 1995: 75: 4744