| Observation Of The Dislocation Structure In [013] Copper Single Crystal During Corrosion Fatigue In Nacl Aqueous Solution |
| YANG Jihong;JIA Weiping; LI Shouxin |
| Department of Physics; Shenyang Normal University |
|
Cite this article:
YANG Jihong; JIA Weiping; LI Shouxin. Observation Of The Dislocation Structure In [013] Copper Single Crystal During Corrosion Fatigue In Nacl Aqueous Solution. Acta Metall Sin, 2004, 40(1): 99-102 .
|
|
|
Abstract The saturation dislocation microstructures in a [013] orientated coppersingle crystal during fatigue in air and NaCl aqueous solutionwere observed by electron channelingcontrast (ECC) technique in SEM and TEM. The resultsshow that the saturation dislocationstructure during the corrosion fatigue in the aqueous solution of 0.5 mol/L NaCl mainly consists of labyrinth and veins dislocation structures, which differs from the dislocation structures of the PSBs and veins in the air environment. The observation reveals that the influence of environment for fatigued dislocation structures is equivalent to increase the plastic shear strain amplitude to the
fatigued sample when other conditions are identical.
|
|
Received: 01 January 1900
|
|
|
[1] Laird C, Charsley P, Mugrabi H. Mater Sci Eng, 1986; 81A: 433 [2] Basinski Z S, Basinski S J. Progr Mater Sci, 1992: 36: 89 [3] Yang J H, Li Y, Li S X, Ma C X, Li G Y. Mater Sci Eng, 2001; 299A: 51 [4] Yang J H, Li Y, Cai Z, Li S X, Ma C X, Ke W. Mater Sci Eng, 2003; 345A: 164 [5] Yang J H, Li S X, Li Y, Han E H, Zhu Z Y, Ke W. Progr Nature Sci, 2002; 12(6) : 454 [6] Yang J H, Li Y, Li S X, Ma C X, Li G Y. Acta Metall Sin, 2000; 36: 1015(杨继红,李勇,李守新,马常祥,李广义.金属学报,2000;36:1015) [7] Yang G H, Ma C X, Li S X. J Northeastern Univ, 2001; 22: 229(杨继红,马常祥,李守新.东北大学学报,2001,22:229) [8] Yang J H, Li Y, Li S X, Ma C X, Li G Y, Wang G, Ke W. Acta Metall Sin, 2001, 37: 507(杨继红,李勇,李守新,马常祥,王刚,柯伟.金属学报,2001;37:507) [9] Yang J H, Li S X, Han E H, Ke W, Zhu Z Y, Li Y, Cai Z. Progr Nature Sci, 2002; 12:77(杨继红,李守新,韩恩厚,柯伟,朱自勇,李勇,蔡正.自然科学进展,2002;12:77) [10] Basinski Z S, Korbel A S, Basinski S J. Acta Metall, 1980; 28: 191 [11] Mughrabi H. Acta Metall, 1983; 31: 1367 [12] Ackermann F, Kubin L P, Lepinoux J, Mughrabi H. Acta Metall, 1984; 32: 715 [13] Hahn H N, Duquette D J. Acta Metall, 1978; 26: 279 [14] Yah B D, Farrington G C, Laird C. Acta Metall, 1985; 33: 1533. [15] Yan B D, Farrington G C, Laird C. Acta Metall, 1985; 33: 1593. [16] Yan B D, Farrington, G C, Laird C. Metall Trans, 1985; 16A: 1151 [17] Ortner S, Laird C, Farrington G C. Acta Metall, 1987; 35: 453 [18] Ortner S, Laird C, Farrington G C. Acta Metall, 1987; 35: 867 [19] Mughrabi H. Mater Sci Eng, 1978; 33: 207 [20] Woods P J. Philos Mag, 1973; 28: 155 [21] Winter A T. Philos Mag, 1974; 29: 719 [22] Finney J M, laird C. Philos Mag, 1975; 31: 339. |