| Corrosion Morphology Diagnosing Syste Of Metallic Materials In Seawater Based On Fractal |
| WANG Shouyan;SONG Shizhe |
| School of Materials; Tianjin University |
|
Cite this article:
WANG Shouyan; SONG Shizhe. Corrosion Morphology Diagnosing Syste Of Metallic Materials In Seawater Based On Fractal. Acta Metall Sin, 2004, 40(1): 94-98 .
|
|
|
Abstract The theory of fractal geometry is used to analyze the corrosion morphology images, which were acquired by scanner. The fractal dimension, generalized dimension, area factor and laucinarity of metallic corrosion images of samples that exposed in seawater were calculated. Taking the obtained characters of metallic samples and their corrosion modality as the knowledge base, the diagnosing system identifying corrosion modality of metallic material in seawater was established according to the theory of fuzzy pattern recognition. The morphology of corrosion images can be identified by acquired fractal characters.
|
|
Received: 16 January 2003
|
|
|
[1] Zhang K H, Wang J R, Zhang Q H. Opto-Electronic Eng, 2001; 28: 52(张坤华,王敬儒,张启衡.光电工程,2001;28:52) [2] Mandelbrot B B, Passoja D E, Paullay A J. Nature, 1984; 308: 721 [3] Costa J M, Sagues F, Vilarrasa M. Corrs Sci, 1991; 32: 665 [4] Chen J, Long Q Y, Chen J Z, Long Q W. J Chin Soc Corros Protect, 1991; 4: 344(陈军,龙起易,陈继志,龙期威.中国腐蚀与防护学报,1991;4:344) [5] Jiang X G, Chu W Y, Xiao J M. J Chin Soc Corros Protect, 1995; 15: 57(蒋兴钢,褚武扬,肖纪美.中国腐蚀与防护学报,1995;15:57) [6] Dong S H, Lv Y M: J Chin Soc Corros Protect, 2001; 2: 106(董绍华,吕英民.中国腐蚀与防护学报,2001;21:106) [7] Dong L K. Theory and Application of Fractal. Shengyang: Liaoning Science and Technology Press, 1990: 174(董连科.分形理论及其应用,沈阳:辽宁科学技术出版社,1990:174) [8] Niruparm S, Chaudhuri B B. Sign Process, 1995; 42: 181 [9] Li K H, Liu Z K, Lin F. J Remot Sens, 2001; 5: 353(李厚强,刘政凯,林峰.遥感学报,1995,5:353) [10] Chaudhuri B, Sarkar N. IEEE Trans Pattern Anal Mach Intellig, 1995; 17: 72 [11] Wang S Y, Kong D Y, Song S Z. Acta Metall Sin, 2001; 37: 517(王守琰,孔德英,宋诗哲.金属学报,2001;37:517) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|