| Influence Of High Temperature Heat Treatment On Microstructure And Microhardness Of (Ds)Nial--Cr(Mo)—Hf Eutectic Alloy |
| XU Chunmei; GUO Jianting |
| Institute of Metal Research; The Chinese Academy of Sciences |
|
Cite this article:
XU Chunmei; GUO Jianting. Influence Of High Temperature Heat Treatment On Microstructure And Microhardness Of (Ds)Nial--Cr(Mo)—Hf Eutectic Alloy. Acta Metall Sin, 2004, 40(1): 57-61 .
|
|
|
Abstract The influence of high temperature heat treatment on microstructure and microhardness of (DS)NiAl--Cr(Mo)--Hf eutectic alloy fabricated with directional solidification under high temperature gradient was investigated. The results indicate that there is little change in the morphology of NiAl and Cr(Mo) phases after high temperature heat treatment. But the semicontinuous Heusler phase which is originally located on the grain boundaries is partially reduced and fine Heusler particles re--precipitated within NiAl matrix. Furthermore, NiAl precipitates coarsen in the Cr(Mo) phase and dislocation appears in the Cr(Mo) phase. Microhardness of as--fabricated (DS)NiAl--28Cr--5Mo--1Hf alloy is much higher than that of (DS)NiAl--28Cr--6Mo and basically unchanged after heat treatment
|
|
Received: 08 March 2003
|
|
|
[1] Walter J L, Cline H E. Metall Trans, 1970; 1:1221 [2] Cline H E, Waiter J L. Metall Trans, 1970; 1:2907 [3] Heredia F E, He M Y, Lucas G E, Evans A G, Deve H E, Konitzer D. Acta Metall Mater, 1993; 41:505 [4] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whit tenberger J D. Intermetalics, 1995; 3:99 [5] Polvani R S, Tzeng W S, Strutt P R. Metall Trans, 1976; 7A: 33 [6] Bowman R R, Noebe R D, Raj S V, Locci I E. Metall Trans, 1992; 23A: 1493 [7] Chen R S, Guo J T, Zhou J Y. Mater Lett, 2000; 42:80 [8] Cui C Y, GUO J T. Acta Metall Sin, 1999; 35:477(崔传勇,郭建亭.金属学报,1999;35:477) [9] Qi Y H, Guo J T, Cui C Y, Li G S. Mater Eng, 2001; 7: 15(齐义辉,郭建亭,崔传勇,李谷松.材料工程,2001;7:15) [10] Yang J M, Jeng S M, Bain K, Amato R A. Acta Mater, 1997; 45:295 [11] Cui C Y, Guo J T, Qi Y H, Ye H Q. Intermetallics, 2002; 10:1001 [12] Cui C Y, Chen Y X, Guo J T, Qi Y H, Ye H Q. Mater Sci Eng, 2002; A325:186 [13] Chen X F, Johnson D R, Noebe R D, Oliver B F. J Mater Res, 1995; 10:1159 [14] Jiang D T, Guo J T. Mater Lett, 1998; 36:33 |