CHARACTERISTICS OF A NiAl EUTECTIC ALLOY JJ—3 WITH EXCELLENT PROPERTIES
YUAN Chao, ZHOU Lanzhang, LI Gusong, GUO Jianting
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
Cite this article: 

YUAN Chao, ZHOU Lanzhang, LI Gusong, GUO Jianting. CHARACTERISTICS OF A NiAl EUTECTIC ALLOY JJ—3 WITH EXCELLENT PROPERTIES. Acta Metall Sin, 2013, 49(11): 1347-1355.

Download:  PDF(3070KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

A new NiAl eutectic alloy JJ—3 with excellent comprehensive properties had been successfully developed in China for the potential vanes materials. In this paper, the study results on alloy JJ—3, including the composition, microstructure characteristics, physical, mechanical and chemical properties, and process technologies have been introduced briefly. On the basis of maintaining the low density, the higher melting point and thermal conductivity, the excellent oxidation resistance being peculiar to NiAl alloy, alloy JJ—3 have good high temperature stress—rupture strength, which are almost as the same as those of the advanced directionally solidified superalloys. Meanwhile, alloy JJ—3 possess good weldability and castability, and had already been cast the vanes with the complicated shape. With the excellent comprehensive properties, alloy JJ—3 is very close to practical engineering application, only if the poor ductility at room temperature must be improved in the future.

Key words:  NiAl alloy      eutectic microstructure      comprehensive property     
Received:  07 August 2013     

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2013.00472     OR     https://www.ams.org.cn/EN/Y2013/V49/I11/1347

[1] Darolia R.  JOM, 1991; 43: 44

[2] Noebe R D, Bowman R R, Nathal M V.  Int Mater Rev, 1993; 38: 193
[3] Darolia R, Walston W S, Nathal M V. In: Kissinger R D, Deye D J, Anton D L,Cetel A D, Nathal M V, Pollock T M, Woodford D A eds.,  Superalloys 1996. Warrendale PA: TMS, 1996: 561
[4] Guo J T.  Order Intermetallic Compound NiAl. Beijing: Science Press, 2003: 1
(郭建亭. 有序金属间化合物镍铝合金. 北京: 科学出版社, 2003: 1)
[5] Cotton J D, Noebe R D, Kaufman M J. In: Doralia R, Liu C T, Martin P L eds.,Int Symp on Structure Intermetallics, Warrendale PA: TMS, 1993: 513
[6] Guo J T, Ren W L, Zhou J.  Acta Metall Sin, 2002; 38: 667
(郭建亭, 任维丽, 周健. 金属学报, 2002; 38: 667)
[7] Whittenberger J D, Gaydosh D J, Kumar K S.  J Mater Sci, 1990; 25: 2771
[8] Guo J T, Xing Z P.  J Mater Res, 1997; 12: 1083
[9] Hollad S, dahmen C, Buhrig—Polaczek A. In: Reed R C, Green K A, Caron P,
Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds.,  Superalloys 2008. Warrendale PA:TMS, 2008: 229
[10] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whittenberger J D.Intermetallics, 1995; 3: 99
[11] Guo J T, Cui C Y, Chen Y X, Li D X, Ye H Q.  Intermetallics, 2001; 9: 287
[12] Bei H, George E P.  Acta Mater, 2005; 53: 69
[13] Guo J T, Xie Y, Sheng L Y, Zhou L Z, Liang Y C.  Intermetallics, 2011; 19: 206
[14] Zhou L Z, Guo J T.  Scr Metall, 1999; 42: 139
[15] Guo J T, Du X H, Zhou L Z.  J Mater Sci Forum, 2005; 475—479: 749
[16] Shang Z, Shen J, Zhang J F, Fu H Z.  Mater Rev, 2011; 25(9): 1
(商昭, 沈军, 张建飞, 傅恒志. 材料导报, 2011; 25(9): 1)
[17] Chen R S, Guo J T, Yin W M, Zhou J Y.  Scr Metall, 1999; 40: 209
[18] Guo J T, Du X H, Zhou B D.  Intermetallics, 2002; 10: 435
[19] Guo J T, Wang Z S, Sheng L Y, Zhou L Z, Yuan C, Chen Z G, Song L.Prog Nat Sci—Mater Int, 2012; 22: 414
[20] Cui C Y, Guo J T, Qi Y H, Ye H Q.  Metall Mater Trans, 2001; 42: 1700
[21] High Temperature Material Division, Chinese Metal Society.  China Superalloys Handbook. Beijing:China Standard Press, 2012: 1
(中国金属学会高温材料分会. 中国高温合金手册. 北京: 中国标准出版社, 2012: 1)
[22] Xu C M, Guo J T, Yang F B.  Acta Metall Sin, 2001; 37: 857
(徐春梅, 郭建亭, 杨福宝. 金属学报, 2001; 37: 857)
[23] Xu C M, Guo J T.  Acta Metall Sin, 2002; 38: 673
(徐春梅, 郭建亭. 金属学报, 2002; 38: 673)
[24] Guo J T, Zhang S Z, Yuan C, Zhou W L, Li G S.  J Aero Mater, 2003; 23(suppl): 34
(郭建亭, 张仕臻, 袁超, 周文龙, 李谷松. 航空材料学报, 2003; 23(suppl): 34)
 [25] Ren W L, Guo J T, Li G S, Wu J S.  Mater Lett, 2005; 59: 1533
 [26] Sheng L Y, Guo J T, Ye H Q.  Mater Des, 2009; 30: 964
[1] ZHAO Naiqin, GUO Siyuan, ZHANG Xiang, HE Chunnian, SHI Chunsheng. Progress on Graphene/Copper Composites Focusing on Reinforcement Configuration Design: A Review[J]. 金属学报, 2021, 57(9): 1087-1106.
[2] LI Xiaofei, GUO Xiping. EUTECTIC MICROSTRUCTURE EVOLUTION OF DIRECTIONALLY SOLIDIFIED Nb-Ti-Si BASE ULTRAHIGH TEMPERATURE ALLOY[J]. 金属学报, 2013, 49(7): 853-862.
[3] HOU Jieshan, ZHOU Lanzhang, GUO Jianting, YUAN Chao. APPLICATION OF ARTIFICIAL NEURAL NETWORK FOR PREDICTION OF SUPERPLASTIC  BEHAVIOUR IN NiAl ALLOYS[J]. 金属学报, 2013, 49(11): 1333-1338.
[4] ZHAO Peng LI Shuangming FU Hengzhi. THREE-DIMENSIONAL MICROSTRUCTURE RECONSTRUCTION AND THE EUTECTIC SPACING ADJUSTMENT DURING DIRECTIONAL SOLIDIFICATION OF Al-40%Cu HYPEREUTECTIC ALLOY[J]. 金属学报, 2012, 48(1): 33-40.
[5] XIAO Xuan XIE Yi GUO Jianting. MICROSTRUCTURES AND MECHANICAL PROPERTIES OF DIRECTIONALLY SOLIDIFIED NiAl–Cr(Mo)–Hf(Ho) EUTECTIC ALLOY[J]. 金属学报, 2010, 46(6): 701-707.
[6] QUAN Qiongrui LI Shuangming FU Hengzhi. EFFECT OF AN ABRUPT GROWTH RATE ON PRIMARY Al2Cu PHASE IN DIRECTIONAL SOLIDIFICATION OF Al–40%Cu HYPEREUTECTIC ALLOY[J]. 金属学报, 2010, 46(4): 500-505.
[7] WANG Yong GUO Xiping. EFFECT OF SOLIDIFYING RATE ON INTEGRALLY DIRECTIONALLY SOLIDIFIED MICROSTRUCTURE AND SOLID/LIQUID INTERFACE MORPHOLOGY OF AN Nb–Ti–Si BASE ALLOY[J]. 金属学报, 2010, 46(4): 506-512.
[8] LI Bin;ZHANG Xiumu; SHA Xianwei; LI Yiyi (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: LI Bin; Tel: (024)23843531-55362; Fax: (024)23891320. MOLECULAR DYNAMICS SIMULATION ON TRANSFORMATION PSEUDOELASTICITY IN NiAI ALLOY[J]. 金属学报, 1998, 34(9): 923-927.
[9] QIN Xiaoying; ZHANG Lide; HOU Bihui; LIANG Renyou; JI Xiaoli(Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031)( University of Science and Technology; Hefei 230026 )(Structure Research Laboratory; University of Science and Technology; Hefei 230026 )(Manuscript received 1995-03-13; in revised form 1995-09-18). STRUCTURE AND MAGNETIC CHARACTER OF NANOSTRUCTURED NiAl ALLOY SYNTHESIZED BY INERT-GAS CONDENSATION[J]. 金属学报, 1996, 32(3): 303-307.
[10] LIU Zhenyun; LIN Dongliang; GU Yuefeng (Shanghai Jiaotong Univereity.Shanghai 200030); CAO Peng; LEI Changming; HUANG Boyun (Center South University of Technology; Changsha 410083). SUPERPLASTIC BEHAVIOUR OF NiAl AND Ni3Al DUPLEX ALLOY[J]. 金属学报, 1996, 32(11): 1139-1143.
No Suggested Reading articles found!