Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (9): 971-976    DOI:
Current Issue | Archive | Adv Search |
GRAPHITE NODULAR PHENOMENA DURING THE ESR OF CAST IRON
CHU Shaojun; LIU Haihong; ZHANG Heyi (Metallurgical Engineering College;University of Science and Technology Beijing; Beijing 100083)Correspondent: CHU Shaojun; associate professor; Tel: (010)62332790; Fax: (010)62522845
Cite this article: 

CHU Shaojun; LIU Haihong; ZHANG Heyi (Metallurgical Engineering College;University of Science and Technology Beijing; Beijing 100083)Correspondent: CHU Shaojun; associate professor; Tel: (010)62332790; Fax: (010)62522845. GRAPHITE NODULAR PHENOMENA DURING THE ESR OF CAST IRON. Acta Metall Sin, 1998, 34(9): 971-976.

Download:  PDF(1090KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the principles of the electrochemical modifying treatment for molten cast iron, preparing ductile iron in ESR process tinder D.C. condition without adding spheroidizing inoculant alloys has been studied in laboratory. The key operation of ESR for producing ductile iron is to increase the silicon content of consumable grey iron electrode and use CaF2-based slags containing rare-earth chide or alkaline-earth oxide and magenisium fluoride. Under the condition of D.C. reversed polarity, the anodic corrosion reaction silicon at the consumable electrode tip leads to a decrease of ferrous oxide concentrationin molten slag, therefore, the cathodic reduction of magnesium canon or cerium cation at the interface between slag and metal pool happens easily.A small amout of nodulizing element such as Mg and Ce, being transferred from slag into metal pool make graphite spheroidizing in remelted ingot. This new method of producing ductile iron in ESR process seems to be useful for the development of new metallurgical technology.
Key words:  nodular cast iron      electroslag remelting      electrochemical     
Received:  18 September 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I9/971

11981; 548(Paton E O. Electroslag Metall, Kuev: Science Press, 1981: 548
21983;(4):39(Zhychenko B B,Peschanskij I P. Foundry Production, 1983;(4):39)
31986;(3):51(Grachev B A, Gorelov N A, PavlenkoN S. Iron Steel Metall1986;(3): 51)
4 Chu Shaojun, Liu Haihong. Proceeding on 9th ICVM, San Diego, California, 1988; 621
5储少军.首届全国青年冶金学术会议文集,冶金工业出版社,1990:121(Chu S J.Proceedings of the First National Youth Symposium on Metallurgy, Beijing: Metallurgical industry press, 1990; 121)
6储少军.化工冶金,1989;(1):15(Chu S J.Eng Chem Metall, 1989;(1):15)
7 Kishna Murthy G G, HashamA, Pal U B. Ironmaking Steelmaking,1993; 20: 191
8Speelman J L, Caley W F, Leewis K G. Metall Trans, 1989; 20B:31
[1] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[2] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[3] HUANG Yichuan, WANG Qing, ZHANG Shuang, DONG Chuang, WU Aimin, LIN Guoqiang. Optimization of Stainless Steel Composition for Fuel Cell Bipolar Plates[J]. 金属学报, 2021, 57(5): 651-664.
[4] CHENG Weili, GU Xiongjie, CHENG Shiming, CHEN Yuhang, YU Hui, WANG Lifei, WANG Hongxia, LI Hang. Discharge Performance and Electrochemical Behaviors of the Extruded Mg-2Bi-0.5Ca-0.5In Alloy as Anode for Mg-Air Battery[J]. 金属学报, 2021, 57(5): 623-631.
[5] Canshuai LIU,Zhaohui TIAN,Zhiming ZHANG,Jianqiu WANG,En-Hou HAN. Corrosion Behaivour of X65 Low Carbon Steel During Redox State Transition Process of High LevelNuclear Waste Disposal[J]. 金属学报, 2019, 55(7): 849-858.
[6] Rongyao MA,Changgang WANG,Xin MU,Xin WEI,Lin ZHAO,Junhua DONG,Wei KE. Influence of Hydrostatic Pressure on Corrosion Behavior of Ultrapure Fe[J]. 金属学报, 2019, 55(7): 859-874.
[7] BAI Yang, WANG Zhenhua, LI Xiangbo, LI Yan. Corrosion Behavior of Al(Y)-30%Al2O3 Coating Fabricated by Low Pressure Cold Spray Technology[J]. 金属学报, 2019, 55(10): 1338-1348.
[8] YANG Yulin, MU Zhangyan, FAN Zheng, DAN Zhenhua, WANG Ying, CHANG Hui. Nanoporous Silver via Electrochemical Dealloying and Its Superior Detection Sensitivity to Formaldehyde[J]. 金属学报, 2019, 55(10): 1302-1310.
[9] Li FAN, Haiyan CHEN, Yaohua DONG, Xueying LI, Lihua DONG, Yansheng YIN. Corrosion Behavior of Fe-Based Laser Cladding Coating in Hydrochloric Acid Solutions[J]. 金属学报, 2018, 54(7): 1019-1030.
[10] Jiang XU, Xike BAO, Shuyun JIANG. In Vitro Corrosion Resistance of Ta2N Nanocrystalline Coating in Simulated Body Fluids[J]. 金属学报, 2018, 54(3): 443-456.
[11] Yun SHU, Maocheng YAN, Yinghua WEI, Fuchun LIU, En-Hou HAN, Wei KE. Characteristics of SRB Biofilm and Microbial Corrosionof X80 Pipeline Steel[J]. 金属学报, 2018, 54(10): 1408-1416.
[12] Jun YU, Deping ZHANG, Ruosheng PAN, Zehua DONG. Electrochemical Noise of Stress Corrosion Cracking of P110 Tubing Steel in Sulphur-Containing Downhole Annular Fluid[J]. 金属学报, 2018, 54(10): 1399-1407.
[13] Hongzhong YUAN,Zhiyong LIU,Xiaogang LI,Cuiwei DU. Influence of Applied Potential on the Stress Corrosion Behavior of X90 Pipeline Steel and Its Weld Joint in Simulated Solution of Near Neutral Soil Environment[J]. 金属学报, 2017, 53(7): 797-807.
[14] Qing LI,Zixing WANG,Shuyuan XIE. Research on the Development of Mathematical Model of the Whole Process of Electroslag Remelting and the Process Simulation[J]. 金属学报, 2017, 53(4): 494-504.
[15] Ju KANG,Jichao LI,Zhicao FENG,Guisheng ZOU,Guoqing WANG,Aiping WU. INVESTIGATION ON MECHANICAL AND STRESS CORROSION CRACKING PROPERTIES OF WEAKNESS ZONE IN FRICTION STIR WELDED 2219-T8 Al ALLOY[J]. 金属学报, 2016, 52(1): 60-70.
No Suggested Reading articles found!