ZHANG Zhefeng; WANG Zhongguang; SU Huihe(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: ZHANG Zhefeng Tel: (024)23843531-55225; Fax: (024)23891320. CYCLIC DEFORMATION BEHAVIOR OF A COPPER BICRYSTAL WITH A PERPENDICULAR GRAIN BOUNDARY. Acta Metall Sin, 1998, 34(8): 841-846.
|
|
|
Abstract Based on the observations of slip patterns and saturation dislocation patterns,the cyclic stress-strain response was investigated by cyclically loading a copper bicrystal with a grain boundary perpendicular to the stress axis under constant plastic strain control. The results showed that the cyclic stress-strain (CSS) curve displayed a double plateau region in the plastic strain range of 1.80 × 10-4 - 2.56 × 10-3. The plateau saturation axial stresses were 62 - 64 MPa and 70 - 71 MPa respectively at axial plastic strain range of 1.80× 10-4- 1.35× 10-3 and 2.04× 10-3 - 2.56× 10-3. The effects of component crystal orientation on the slip characteristics, saturation dislocation patterns and CSS curve were discussed.
|
|
Received: 18 August 1998
|
1 Hauser J J, Chalmers B. Acta Metall, 1961; 9: 802 2 Miura S, Hamashima K, Aust K T. Acta Metall 1980; 28: 1591 3 Rey C, Zaoui A. Acta Metall 1980; 28: 687 4 Chuang Y D, Margolin H. Metall Trans, 1973; 3A: 1905 5 Hu Y M, Wang Z G. Int J Fatigue, 1997; 19: 59 6 Hu Y M, Wang Z G. Acta Mater 1997; 45: 2655 7 Peralta P, Laird C. Acta Mater 1997; 45: 3029 8 宫波,苏会和,陈道伦,王中光.金属学报, 1997; 33: 561(Gong B, Su H H, Chen D L, Wang Z G. Acta Metall Sin 1997; 33: 561) 9 胡运明, 陈道伦,苏会和,王中光,材料研究学报, 1997; 11: 240(Hu Y M, Su H H, Chen D L, Wan Z G. Chin J Mater Res, 1997; 11: 240) 10 Zhang Z F, Wang Z G. Philos Mag Lett. 1998, in press 11 Mughrabi H. Mater Sci Eng, 1978; 33: 207 12 Laird C, Charsley P, Mughrabi H. Mater Sci Eng, 1986; 81: 433 13 Winter A T. Philoa Mag 1974; 30: 719 14 Cheng A S, Laird C. Mater Sci Eng, 1981; 51: 111A |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|