| STRUCTURAL CHARACTERIZATION AND INTRINSIC MAGNETIC PROPERLIES OF THE SmFe_(10.7-x)Mo_(1.3)Ga_x COMPOUNDS |
| PAN Hongge; CHEN Yun; CHEN Changpin(Department of Materials Science and Eegineering; Zhejiang University; Hangzhou 310027)YANG Fuming(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)Correspondent: PAN Hongge; Tel: (0571)7951406 Fax: (0571)7951152 |
|
Cite this article:
PAN Hongge; CHEN Yun; CHEN Changpin(Department of Materials Science and Eegineering; Zhejiang University; Hangzhou 310027)YANG Fuming(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)Correspondent: PAN Hongge; Tel: (0571)7951406 Fax: (0571)7951152. STRUCTURAL CHARACTERIZATION AND INTRINSIC MAGNETIC PROPERLIES OF THE SmFe_(10.7-x)Mo_(1.3)Ga_x COMPOUNDS. Acta Metall Sin, 1998, 34(8): 836-840.
|
|
|
Abstract The structural characterization and intrinsic magnetic properties of the compounds SmFe10.7-x Mo1.3Gax have been investigated in great detail, which included the lattice parameters, Curie temperature TC, saturation magnetization σs, and magnetocrystallize anisotropy. The results indicate that Ga occupies 8j and 8f sites, and substitution of Ga for Fe in SmFe10.7Mo1.3 leads to the expansion of the lattice constants a, c and unit cell volume V, the monotonical decrease of the Curie temperature TC, and the decrease of saturation magnetization and the Fe moments. The magnetocrystalline anisotropy changes from uniaxial to conical plane.
|
|
Received: 18 August 1998
|
1 Middleton D F, Mishra S R, Long G J, Pringle O A, Hu Z, Yelon W B, Grandjean F, Buschow K H J.J Appl Phys, 1995; 78: 5568 2 Rogalski M S, Morariu M, Valeanu M, Plugurn N. Solid State Commun, 1993; 87: 139 3 Li Z W, Zhou Z, Morrish A H. Phys Rev, 1995; 51B: 2891 4 Sabirianor R F, Jaswal S S. J Appl Phys, 1996; 79: 5942 5 Coehoorn R. Phys Rev, 1990; 41B: 1790 6 Mooji D B, Buschow K H J. J Less-Common Met, 1988; 131: 207 7 成昭华.中国科学物理研究所博士学位论文, 1995(Chen Z H, Ph D Thesis, Institute of Physics, The Chinese Academy of Sciences, Beijing, 1995)j |