| AN INVESTIGATUIB ON THE RECOVERY BEHMIORS OF THE LATTICE DISTORTIONS IN AN Ni_3P/Ni NANOPHASE MATERIAL |
| SUI Manling(Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Coerespondent: SUI Manling; Fax:(024)3890488; Tel: (024)3893000-7740; E-mail: misui mail.neu.edu.cn |
|
Cite this article:
SUI Manling(Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Coerespondent: SUI Manling; Fax:(024)3890488; Tel: (024)3893000-7740; E-mail: misui mail.neu.edu.cn. AN INVESTIGATUIB ON THE RECOVERY BEHMIORS OF THE LATTICE DISTORTIONS IN AN Ni_3P/Ni NANOPHASE MATERIAL. Acta Metall Sin, 1998, 34(6): 650-654.
|
|
|
Abstract An Ni3P/Ni nanophase material, syathesised by the complete crystallization ofan amorphous Ni--P alloy, has been annealed isothermally at differellt temperatures. Variationsof the lattice parameters of the two nanophases with the annealing temperature/time were detendned by means of quantitative X--ray diffraction measurement. It was found that the latticedistortion of the nanophases was recovered during the annealing treatment, but the recovery behaviors of the two nanophases were obviously different at different annealing temperatures. TheseVariations in the microstructure of the nanophases were interpreted in terms of thermodynamicconsiderations.
|
|
Received: 18 June 1998
|
1 隋曼龄,卢柯 金属学报,1994230:B413 (Su M L,, Lu K. Acta metall Sin, 1994; 30: B413) 2 Liu X D ,Lu K,Ding B Z ,Hu Z Q .Nanostructured Mater 1993;2:581 3 董振富,卢柯,魏文择,丁炳哲 金属学报,1994;30:B304 (Dong Z F, Lu K, Wei W D, Ding B Z. Acta Metall Sin, 1994; 30: B304) 4 Gaffet E, Harmelin M.J Less-comm Metals, 1993; 157: 201 5 卢柯,刘学东,张皓月,胡壮麒 金属学报.1995;31:A74 (Lu K, Liu X D, Zhang H Y, Hu Z Q. Acta Metall Sin , 1995; 31: A74) 6 Lu K, Wang J T, Wei W D.J Appl Phys, 1991; 69: 522 7 Sui M L, Lu K, He Y Z. Philos Mag, 1991; B63: 933 8 Donnay J D H, Ondik H M eds, Crystal Data Determinative Tables ,3rd ,Ed,NBSJCPDS , 1973: 2 9 Cahn R W, Haasen P. Physical Metallurgy, 3rd Ed, Amsterdam: Elsevier Csi Publ, 1983: 980 10 Periodic Table of the Elements, VCH, 1993 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|