| RESEARCH OF GALVANIZED PROCESS OF ELECTROLYTIC COPPER FOIL |
| LENG Daguang;HU Jingjiang;GUO Zongxun;XU Shumin (Zhaoyuan;JINBAO Electronics Co. Ltd; Shandong 265400) |
|
Cite this article:
LENG Daguang;HU Jingjiang;GUO Zongxun;XU Shumin (Zhaoyuan;JINBAO Electronics Co. Ltd; Shandong 265400). RESEARCH OF GALVANIZED PROCESS OF ELECTROLYTIC COPPER FOIL. Acta Metall Sin, 1998, 34(11): 1227-1229.
|
|
|
Abstract This article discusses galvanizing methods adopted sulfate technology and researches a formula and conditions for manufacturing electrolytic copper foil. It shows that the technology can meet quality requirements and has the advantages of a stable process, easy to operate and a low cost. It is an ideal manufacturing process of galvanizing copper foil.
|
|
Received: 18 November 1998
|
1 张继世,刘江金属表面工艺.北京:机械工业出版社,1995:75(Zhan J S, Liu J.Technology of Metal Surface.Bejing:Machinery Industry Press,1995:75) 2 朱庚惠,谭亮,朱修业,李静波.中级电镀工工艺学.北京:机械工业出版社,1988:54(Zhu G H,Tan L,Zhu X Y,Li J B.Middle Plating Technology.Bejing:Machinery Industry Press,1988:54 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|