| STUDY ON THERMODYNAMICAL PROPERTIES IN Mn-Fe ALLOY MELTS |
| CHEN Erbao; DONG Yuanchi; GUO Shangxing (EaSt China Institute of Metallurgy; Ma'anshan 243002) (Manuscript received 1996-09-15; in revised form 1996-11-25) |
|
Cite this article:
CHEN Erbao; DONG Yuanchi; GUO Shangxing (EaSt China Institute of Metallurgy; Ma'anshan 243002) (Manuscript received 1996-09-15; in revised form 1996-11-25). STUDY ON THERMODYNAMICAL PROPERTIES IN Mn-Fe ALLOY MELTS. Acta Metall Sin, 1997, 33(8): 831-837.
|
|
|
Abstract The solubility of carbon in Mn-Fe alloy melts was measured experimentally at 1400 ℃. The solubility of carbon in Mn-Fe alloy melts (from pure Mn to pure Fe) can be cal-culated with following formula: Xc=0.1886+0.1 119XMn or XC=0.2703-0.1006XFe. By thermodynamical derivation and calculation, some thermodynamical data were obtained as follows: 1) in Fe-C and Fe-Mn-C systems, lnγ℃= -0.033, ε= 9.02, eg= 0.1534, in Mn-C and Mn-Fe-C systems,
|
|
Received: 18 August 1997
|
1倪瑞明,马中庭,魏寿昆.钢铁研究学报,1990;4:17 2郭上型,董元篪.金属学报, 1995; 31: B241 3 Turkdogan E T,Leake L E.J Iron Steel Inst,1995;179:39 4魏寿昆.冶金过程热力学上海:上海科学技术出版社,1980:388 5黄希祜.钢铁冶金原理(修订版).北京:冶金工业出版社,1990:58 6 Chipman J.Metall Trans,1970;1:2163 7上田 阳.铁钢,1975;61:2692 8 Lupis C H P.Acta Metall, 1968;16:1365< |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|