Please wait a minute...
Acta Metall Sin  1997, Vol. 33 Issue (5): 492-498    DOI:
Current Issue | Archive | Adv Search |
MULTI-COMPONENT MICRO-ALLOYED AIR COOLING BAINITIC STEELS
LI Fengzhao;GU Yingni;JIANG Jiang;AO Qing;SUN Dongsheng (College of Materials Science and Engineering; Shandong University of Technology; Jinan 250061)
Cite this article: 

LI Fengzhao;GU Yingni;JIANG Jiang;AO Qing;SUN Dongsheng (College of Materials Science and Engineering; Shandong University of Technology; Jinan 250061). MULTI-COMPONENT MICRO-ALLOYED AIR COOLING BAINITIC STEELS. Acta Metall Sin, 1997, 33(5): 492-498.

Download:  PDF(3843KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Medium carbon and medium-high carbon air cooling micro-alloyed bainitic steels of Mn-Si-B system have been studied. The main structure is bainite or bainite/martensite after forging and air cooling, and there are carbides and a small amount of retained austenite. The structure is fine and uniform, and the addition of micro-amount elements can further refine the austenite grain and the bainitic structure.By modified treatments of mono, binary and ternary micro-alloying, the structures of various grades can be obtained, and their hardness, toughness and wear resistance increase successively. The structure of the air cooling bainitic steels with medium high carbon treated by ternary micro-alloyed after forging and tempering or nomalizing and tempering is much finer, the properties are much superior.
Key words:  micro-alloyed bainitic steel      structure finning      wear resistance     
Received:  18 May 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I5/492

1 Irvine K J,Pickering F B.J Iron Steel Inst,1957;87:292
2 Bhadeshia H K O H.Bainite in Steels.London:the Institute of Materials,1992:348,380
3刘晓,张明星,陈大明,周鹿宾,康沫狂.金属学报,1993;29:A97
4赵如发,方鸿生,郑燕康,陈秀云.中国专利 86 103 009,1987
5方鸿生,郑燕康,陈秀云,黄云庆,曹建军,姜忠良.中国机械工程学会第二届材料年会论文集,1990:11,115
[1] WANG Haifeng, ZHANG Zhiming, NIU Yunsong, YANG Yange, DONG Zhihong, ZHU Shenglong, YU Liangmin, WANG Fuhui. Effect of Pre-Oxidation on Microstructure and Wear Resistance of Titanium Alloy by Low Temperature Plasma Oxynitriding[J]. 金属学报, 2023, 59(10): 1355-1364.
[2] ZHANG Yu, LOU Liyan, XU Qinglong, LI Yan, LI Changjiu, LI Chengxin. Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding[J]. 金属学报, 2020, 56(11): 1530-1540.
[3] Hulin DONG,Haiping BAO,Jianhong PENG. Effect of TiC Contents on Mechanical Properties and Wear Resistance of Iron-Based Composites[J]. 金属学报, 2019, 55(8): 1049-1057.
[4] Shilu ZHAO,Zhen ZHANG,Jun ZHANG,Jianming WANG,Zhenggui ZHANG. MICROSTRUCTURE AND WEAR RESISTANCE OF TiAlZrCr/(Ti, Al, Zr, Cr)N GRADIENT FILMS DEPOSITED BY MULTI-ARC ION PLATING[J]. 金属学报, 2016, 52(6): 747-754.
[5] Wenfang CUI,Dong CAO,Gaowu QIN. MICROSTRUCTURE AND WEAR RESISTANCE OF Ti/TiN MULTILAYER FILMS DEPOSITED BY MAGNETRON SPUTTERING[J]. 金属学报, 2015, 51(12): 1531-1537.
[6] LIU Xiaobo, ZHAO Yuguang. MICROSTRUCTURE EVOLUTION AND WEAR RESISTANCE OF IN SITU Mg2Si/Al COMPOSITES UNDER DIFFERENT PREPARATION CONDITIONS[J]. 金属学报, 2014, 50(6): 753-761.
[7] NIU Yunsong, WEI Jie, ZHAO Jian, HU Jiaxiu, YU Zhiming. PREPARATION AND PROPERTIES OF NANOSIZED MUL-TILAYERED Ni COATINGS BY ULTRASOUND-ASSISTED ELECTRODEPOSITION[J]. 金属学报, 2013, 49(12): 1617-1622.
[8] YU Yipeng HUANG Jinfeng CUI Hua CAI Yuanhua ZHANG Jishan. EFFECT OF Nb ON THE MICROSTRUCTURE AND PROPERTIES OF SPRAY FORMED M3 HIGH SPEED STEEL[J]. 金属学报, 2012, 48(8): 935-940.
[9] ZHANG Fenggang ZHU Xiaopeng WANG Mingyang LEI Mingkai. SURFACE MODIFICATION OF WC-Ni CEMENTED CARBIDE FOR SEALS BY HIGH-INTENSITY PULSED ION BEAM IRRADIATION[J]. 金属学报, 2011, 47(7): 958-964.
[10] WANG Yanqiu WANG Yue CHEN Paiming SHAO Yawei WANG Fuhui. MICROSTRUCTURE, CORROSION AND WEAR RESISTANCES OF MICROARC OXIDATION COATING ON Al ALLOY 7075[J]. 金属学报, 2011, 47(4): 455-461.
[11] LEI Mingkai WANG Kesheng OU Yi Xiang ZHANG Lei. PLASMA–BASED LOW–ENERGY NITROGEN ION IMPLANTATION OF 2Cr13 MARTENSITIC STAINLESS STEEL USED IN PUMPS AND VALVES[J]. 金属学报, 2011, 47(12): 1490-1494.
[12] LI Jian; MAO Dongsheng; HUANG Liping; GUO Shaoyi; MAO Zhiyuan(Department of Materials Science and Engineering; Zhejiang University Hangzhou 310027Ion Beam Laboratory; Shanghai Institute of Metallurgy The Chinese Academy of Sciences; Shanghai 200050). PROPERTIES AND ABRASION WEAR RESISTANCE OF AN Al_2O_3-TiC-Co MODIFIED CERAMIC[J]. 金属学报, 1998, 34(3): 332-336.
[13] WANG Huaming(H.M.Wang)(Beijing University of Aeronautics and Astronautics; Beijing 100083). SURFACE MODIFICATION OF TiAl INTERMETALLIC ALLOYS BY LASER GAS ALLOYING[J]. 金属学报, 1997, 33(9): 917-920.
[14] WU Ping; ZHOU Changzhi; TANG Xi'nan (Tsinghua Univereity; Beijing)(Manuscript received 11 April;1994). PREPARATION OF WEAR-RESISTANT GRADED METAL-CERAMIC COATING BY LASER-ALLOYING[J]. 金属学报, 1994, 30(23): 508-512.
[15] XU Yourong;ZHANG Henghua;CHEN Daming;XIE Fuchun;XU Mingyu;CHEN Lanying;SU Baorong;QIAN Hongbin Shanghai University of Science and Technology Shanghai Optics and Fine Mechinery Research Institute; Academia Sinica professor;Department of Materials Science and Engineering;Shanghai University of Science and Technology; Shanghai 201800. EFFECT OF LASER SCANNING SPEED ON PHASE CONSTITUTION AND WEAR RESISTANCE OF LASERCLADDING STELLITE HARD FACING ALLOY[J]. 金属学报, 1993, 29(3): 30-34.
No Suggested Reading articles found!