ALLOYING BEHAVIOUR OF Mg, Ca,Y, La AND Ce IN Ni_3Al
ZHANG Yun; LIN Dongliang; HUANG Jin (Shanghai Jiaotong University; Shanghai 200030)
Cite this article: 

ZHANG Yun; LIN Dongliang; HUANG Jin (Shanghai Jiaotong University; Shanghai 200030). ALLOYING BEHAVIOUR OF Mg, Ca,Y, La AND Ce IN Ni_3Al. Acta Metall Sin, 1997, 33(3): 259-264.

Download:  PDF(487KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The alloying behavioUrs of Mg, Ca, Y, La and Ce in Ni3Al have been determined by X-ray diffraction measurement. It is found that Mg, Ca, Y, La and Ce atoms occupy the Al site in the L12structure. Besides, the additive atoms can further increase the long-range order degree for Ni3Al and this increment becomes more pronounced in the sequence of Mg, Ca, Y(La-Ce). Finally, the lattice parameters of the Ni3Al alloys with the alloy additions have also been determined. It is found that the lattice parameters of Ni3Al increase linearly with increasing elemental content. and this increment becomes more pronounced in the sequence of Ma, Ca. Y, La-Ce.
Key words:  intermetallics      Ni_3Al      solid solution alloying      lattice parameter     
Received:  18 March 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I3/259

1 Han K H, Choo W K Scr Metall. 1983;17: 281
2 Masahashi N, Takasugi T,Izumi O. Acta Metall , 1988: 36:1815
3 Foiles S M,Daw M S.J Mater Res,1987;2:5
4 Miedema A R,Chatel P F.In:Benett L H ed,Theory of Alloy Phase Formation,New York:AIML.1980:304
5王崇愚,刘森英中国科学,1991;A(6):647D
[1] GONG Shengkai, SHANG Yong, ZHANG Ji, GUO Xiping, LIN Junpin, ZHAO Xihong. Application and Research of Typical Intermetallics-Based High Temperature Structural Materials in China[J]. 金属学报, 2019, 55(9): 1067-1076.
[2] Lin GENG, Hao WU, Xiping CUI, Guohua FAN. Recent Progress on the Fabrication of TiAl-Based Composites Sheet by Reaction Annealingof Elemental Foils[J]. 金属学报, 2018, 54(11): 1625-1636.
[3] Xuan YU, Zhihao ZHANG, Jianxin XIE. Microstructure, Ordered Structure and Warm TensileDuctility of Fe-6.5%Si Alloy with Various Ce Content[J]. 金属学报, 2017, 53(8): 927-936.
[4] Li ZHOU,Chao CUI,Qing JIA,Yingshi MA. Experimental and Finite Element Simulation of Milling Process for γ-TiAl Intermetallics[J]. 金属学报, 2017, 53(4): 505-512.
[5] Jihou LIU,Hongyun ZHAO,Zhuolin LI,Xiaoguo SONG,Hongjie DONG,Yixuan ZHAO,Jicai FENG. Microstructures and Mechanical Properties of Cu/Sn/Cu Structure Ultrasonic-TLP Joint[J]. 金属学报, 2017, 53(2): 227-232.
[6] Guotian WANG, Hongsheng DING, Ruirun CHEN, Jingjie GUO, Hengzhi FU. Effect of Current Intensity on Microstructure of Ni3Al Intermetallics Prepared by Directional Solidification Electromagnetic Cold Crucible Technique[J]. 金属学报, 2017, 53(11): 1461-1468.
[7] Tong LIU,Liangshun LUO,Yanning ZHANG,Yanqing SU,Jingjie GUO,Hengzhi FU. MICROSTRUCTURE EVOLUTION AND GROWTH BEHAVIORS OF FACETED PHASE IN DIRECTIONALLYSOLIDIFIED Al-Y ALLOYS II. Microstructure Evolution of Directionally Solidified Al-53%Y Peritectic Alloy[J]. 金属学报, 2016, 52(7): 866-874.
[8] TIAN Sugui, WANG Xin, XIE Jun, LIU Chen, GUO Zhongge,LIU Jiao, SUN Wenru. CHARACTERISTIC AND MECHANISM OF PHASE TRANSFORMATION OF GH4169G ALLOY DURING HEAT TREATMENT[J]. 金属学报, 2013, 49(7): 845-852.
[9] PENG Yingbo, CHEN Feng, WANG Minzhi, SU Xiang, CHEN Guang. RELATIONSHIP BETWEEN MECHANICAL PROPERTIES AND LAMELLAR ORIENTATION OF PST CRYSTALS IN Ti-45Al-8Nb ALLOY[J]. 金属学报, 2013, 49(11): 1457-1461.
[10] LIANG Yongchun GUO Jianting; SHENG Liyuan; ZHOU Lanzhang. EFFECTS OF RARE EARTH ELEMENT Gd ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF NiAl-Cr(Mo)-Hf EUTECTIC ALLOY[J]. 金属学报, 2010, 46(5): 528-532.
[11] ZHOU Minbo LI Xunping MA Xiao ZHANG Xinping. EARLY INTERFACIAL REACTION AND UNDERCOOLING SOLIDIFICATION BEHAVIOR  OF Sn-3.5Ag/Cu SYSTEM[J]. 金属学报, 2010, 46(5): 569-574.
[12] ZHOU Dianwu XU Shaohua ZHANG Fuquan PENG Ping LIU Jinshui. FIRST-PRINCIPLES CALCULATIONS OF STRUCTURAL STABILITIES AND ELASTIC PROPERTIES OF AB2 TYPE INTERMETALLICS IN ZA62 MAGNESIUM ALLOY[J]. 金属学报, 2010, 46(1): 97-103.
[13] ZHAO Yufei FU Yuechun HU Qingmiao YANG Rui. FIRST-PRINCIPLES INVESTIGATIONS OF LATTICE PARAMETERS, BULK MODULI AND PHASE STABILITIES OF Ti1-xVx AND Ti1-xNbx ALLOYS[J]. 金属学报, 2009, 45(9): 1042-1048.
[14] HU Jing LIN Dongliang WANG Yan. EBSD ANALYSES OF THE MICROSTRUCTURAL EVOLUTION AND CSL CHARACTERISTIC GRAIN BOUNDARY OF COARSE--GRAINED NiAl ALLOY DURING PLASTIC DEFORMATION[J]. 金属学报, 2009, 45(6): 652-656.
[15] HE Hongwen XU Guangchen GUO Fu. FORMATION OF WHISKER AND HILLOCK IN Cu/Sn--58Bi/Cu SOLDERED JOINT DURING ELECTROMIGRATION[J]. 金属学报, 2009, 45(6): 744-748.
No Suggested Reading articles found!