THE CORROSIVE WEAR BEHAVIOR OF Cr-Mn-N SERIES CASTING STAlNLESS STEEL |
BI Hongyun; JIANG Xiaoxia; LI Shizhuo;YANG Jingxian(Institute of Metal Research; Chinese academy of Sciences; Shenyang 110015)(Shenyang Polytechnic University; Shenyang 110023) |
|
Cite this article:
BI Hongyun; JIANG Xiaoxia; LI Shizhuo;YANG Jingxian(Institute of Metal Research; Chinese academy of Sciences; Shenyang 110015)(Shenyang Polytechnic University; Shenyang 110023). THE CORROSIVE WEAR BEHAVIOR OF Cr-Mn-N SERIES CASTING STAlNLESS STEEL. Acta Metall Sin, 1997, 33(10): 1069-1074.
|
Abstract The corrosive wear behavior of Cr-Mn-N casting stainless steel with addition of Cu and Mo in media of H2SO4, HNO3, HaC acid is investigated. Its corrosive wear resistance is much better than that of 304 stainless steel. and the reason is that, besides the similar corrosive resistance between Cr-Mn-N casting stainless steel and 304 stainless steel, the former has a better work-hardening ability than that of Ni series stainless steel in wear experiment. So it is fit for dominative wear condition.
|
Received: 18 October 1997
|
1铬锰氮无镍不锈钢的研究.中国科学院金属研究所,1969 2姜晓霞,李诗卓,陶冬东,杨景样.材料科学进展.1992;6:199 3路新春,姜晓霞,李诗卓,张天成.中国腐蚀与防护学报.1994;14:201 4李诗卓,姜晓霞.腐蚀科学与防护技术.1995;7:122 5Jian X X Li S Z Tao D D Yang J X. Corrosion 1993; 49: 836 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|