| EFFECT OF HYDROGEN ON IRRADIATION SWELLING IN FERRITIC STEEL |
| WAN Farong; HUANG Xuejun; CHU Wuyang; XIAO Jimei(University of Science and Technology Beijing; 100083)(Manuscript received 93-11-09; in revised form 94-04-11) |
|
Cite this article:
WAN Farong; HUANG Xuejun; CHU Wuyang; XIAO Jimei(University of Science and Technology Beijing; 100083)(Manuscript received 93-11-09; in revised form 94-04-11). EFFECT OF HYDROGEN ON IRRADIATION SWELLING IN FERRITIC STEEL. Acta Metall Sin, 1995, 31(2): 69-73.
|
|
|
Abstract JFMS alloy specimens were implanted with hydrogen ion by ion accelerator.and then electron irradiated by HVEM.The results showed that hydrogen implantation promotes the void nucleation under electron irradiation at above 570 K. At 670 K, the void number density in the specimen with hydrogen would be one order of magnitude higher than the specimen without hydrogen. Void swelling would also increase by hydrogen implantation.Correspondent WAN Farong. associate peo fessor,Department of Materials Physics, University of Science andTechnology Beijing, Beijing 100083
|
|
Received: 18 February 1995
|
| 1MaziaszPJ.ORNL-6721,19852MurphySM.JNuclMater,1988;155-157:8663TakeyamaT,OhnukiS,TakahashiH,WanF.In:HashigutiRReds.,ProgressinMetalPhysicsandPhysicalMetallurgy,Tokyo:BusinessCenterforAcademicSociety,1986:154MyersSM,MaterSciEng,1985;69:3978 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|