Acta Metall Sin  1995, Vol. 31 Issue (17): 220-225    DOI:
Current Issue | Archive | Adv Search |
PREPARATION OF BULK Al-Fe(MO, Si, B)NANOSTRUCTURED ALLOY BY DIFFUSION REACTION UNDER HIGH PRESSURE
YAO Bin; (Institute of Metal Research; Chinese A cademy of Sciences; Shenyang 110015)DING Bingzhe; LI Dongjian; WANG Aimin; HU Zhuangqi (State Key Laberatory for RSA; Institute of Metal Research; Chinese Acadeimy of Sciences; Shenyang 110015)(Siping Normal College; Siping 136000)
Cite this article: 

YAO Bin; (Institute of Metal Research; Chinese A cademy of Sciences; Shenyang 110015)DING Bingzhe; LI Dongjian; WANG Aimin; HU Zhuangqi (State Key Laberatory for RSA; Institute of Metal Research; Chinese Acadeimy of Sciences; Shenyang 110015)(Siping Normal College; Siping 136000). PREPARATION OF BULK Al-Fe(MO, Si, B)NANOSTRUCTURED ALLOY BY DIFFUSION REACTION UNDER HIGH PRESSURE. Acta Metall Sin, 1995, 31(17): 220-225.

Download:  PDF(438KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study on the diffusion reaction of melted Al and (Fe0.99, Mo0.01)78Si9B13 amopohous alloy was carried out under a pressure of 3 GPa at temperature ranging from 570 to 850℃. A bulk Al-Fe(Mo,Si,B) nanostructured alloy composed of a single phase was prepared by heating alternate layers of (Fe0.99, M0.01)78S9B13 amorphous ribbons and pure Al sheets for 20 min under a pressure of 3 GPa at temperatures of 800 to 830℃. Its mean grain size is 22 nm and its lattice is orthorhombic. Its thermostability is fairly good and its hardness is 6.9 GPa.
Key words:  diffusion reaction      nanostructured alloy      high pressure     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I17/220

1BirringerR,HerrU,GleiterH.SupplTransJpnInstMet.1986;27:432QiXY,WuWJ,ChengLF.NanostructMater,1993;2(1):993HahnH,LogasJ,AverbackRS.JMalerRes,1990;5(3):6094UhlmannDR,HaysJF,TurnbullD.PhysChemGlasses.,1966;7(5):1595StrozkajaGG.Ph.Dthesis,HighPressurePhysicsInstitute,Moscow,19886XuY,HuangX,WangWK.ApplPhysLett,1990;56:19577LarchevVT,MelnikNN,PopovaSV,StrotskayaGG,TalenskijON.ProcLebedev,PhysInstitute,1985;1:7(inRussian)8姚斌,张强,苏文辉.高压物理学报,1990;4(1):509LiDJ,DingBZ,YaoB,HuZQ.NanostructMuter,1994;4:32310汪复兴主编.金属物理.北京:机械工业出版社,1981:167
[1] CAO Shuting, ZHANG Shaohua, ZHANG Jian. Combustion Behavior of GH4061 Alloy in High Pressure and Oxygen-Enriched Atmosphere[J]. 金属学报, 2023, 59(4): 547-555.
[2] WANG Tao, LONG Dijun, YU Liming, LIU Yongchang, LI Huijun, WANG Zumin. Microstructure and Mechanical Properties of 14Cr-ODS Steel Fabricated by Ultra-High Pressure Sintering[J]. 金属学报, 2022, 58(2): 184-192.
[3] LI Xiaohui, WANG Jianqiu, HAN En-Hou, GUO Yanjun, ZHENG Hui, YANG Shuangliang. Electrochemistry and In Situ Scratch Behavior of 690 Alloy in Simulated Nuclear Power High Temperature High Pressure Water[J]. 金属学报, 2020, 56(11): 1474-1484.
[4] Ping LI, Quan LIN, Yufeng ZHOU, Kemin XUE, Yucheng WU. TEM Analysis of Microstructure Evolution Process of Pure Tungsten Under High Pressure Torsion[J]. 金属学报, 2019, 55(4): 521-528.
[5] Shoumei XIONG, Jinglian DU, Zhipeng GUO, Manhong YANG, Mengwu WU, Cheng BI, Yongyou CAO. Characterization and Modeling Study on Interfacial Heat Transfer Behavior and Solidified Microstructure of Die Cast Magnesium Alloys[J]. 金属学报, 2018, 54(2): 174-192.
[6] Lining XU,Bei WANG,Minxu LU. CORROSION BEHAVIOR OF 6.5%Cr STEEL IN HIGH TEMPERATURE AND HIGH PRESSURE CO2 ENVIRONMENT[J]. 金属学报, 2016, 52(6): 672-678.
[7] Jianqiu WANG, Fa HUANG, Wei KE. CORROSION BEHAVIORS OF INCONEL 690TT AND INCOLOY 800MA STEAM GENERATOR TUBES IN HIGH TEMPERATURE HIGH PRESSURE WATER[J]. 金属学报, 2016, 52(10): 1333-1344.
[8] Yongyou CAO, Shoumei XIONG, Zhipeng GUO. DEVELOPMENT OF AN INVERSE HEAT TRANSFER MODEL BETWEEN MELT AND SHOT SLEEVE AND ITS APPLICATION IN HIGH PRESSURE DIE CASTING PROCESS[J]. 金属学报, 2015, 51(6): 745-752.
[9] JIE Jinchuan, ZOU Chunming, WANG Hongwei, WEI Zunjie. MECHANICAL BEHAVIOR OF Al-20Mg ALLOY SOLIDIFIED UNDER HIGH PRESSURE[J]. 金属学报, 2014, 50(8): 971-978.
[10] DONG Yun, LIN Xiaoping, XU Rui, FAN Zhibin, YE Jie, WANG Zhe. MICROSTRUCTURE AND ROOM TEMPERATURE COMPRESSION PROPERTIES OF Mg82.13Zn13.85Y4.02 ALLOY SOLIDIFIED UNDER SUPER-HIGH PRESSURE[J]. 金属学报, 2014, 50(5): 594-600.
[11] ZHANG Litao,WANG Jianqiu. STRESS CORROSION CRACK PROPAGATION BEHAVIOR OF DOMESTIC FORGED NUCLEAR GRADE 316L STAINLESS STEEL IN HIGH TEMPERATURE AND HIGH PRESSURE WATER[J]. 金属学报, 2013, 49(8): 911-916.
[12] LI Xiaohui WANG Jianqiu HAN En–Hou KE Wei. CORROSION BEHAVIOR OF NUCLEAR GRADE ALLOYS 690 AND 800 IN SIMULATED HIGH TEMPERATURE AND HIGH PRESSURE PRIMARY WATER OF PRESSURIZED WATER REACTOR[J]. 金属学报, 2012, 48(8): 941-950.
[13] LI Xiaohui HUANG Fa WANG Jianqiu HAN En-Hou KE Wei. INFLUENCES OF TiN INCLUSION ON CORROSION AND STRESS CORROSION BEHAVIORS OF ALLOY 690 TUBE IN HIGH TEMPERATURE AND HIGH PRESSURE WATER[J]. 金属学报, 2011, 47(7): 847-852.
[14] KUANG Wenjun WU Xinqiang HAN En-Hou. EFFECT OF Ni2+ IN OCCLUDED VOLUME ON THE OXIDATION BEHAVIOR OF 304 STAINLESS STEEL IN HIGH TEMPERATURE WATER[J]. 金属学报, 2011, 47(7): 927-931.
[15] WU Mengwu XIONG Shoumei. EXPERIMENTAL AND MODELING STUDIES ON THE STRUCTURE FORMATION OF HIGH PRESSURE DIE CAST MAGNESIUM ALLOY CONSIDERING THE EXTERNALLY SOLIDIFIED CRYSTALS IN THE SHOT SLEEVE\par[J]. 金属学报, 2011, 47(5): 528-534.
No Suggested Reading articles found!