| AN OVERVIEW OF RECENT PROCESSES AND ARGUMENTS ON BAINITIC TRANSFORMATION THEORY |
| FANG Hongsheng;WANG Jiajun (Tsinghua University; Beijing)(Manuscript received 25 March; 1994) |
|
Cite this article:
FANG Hongsheng;WANG Jiajun (Tsinghua University; Beijing)(Manuscript received 25 March; 1994). AN OVERVIEW OF RECENT PROCESSES AND ARGUMENTS ON BAINITIC TRANSFORMATION THEORY. Acta Metall Sin, 1994, 30(11): 481-490.
|
|
|
Abstract The main points of view about shear and difusion for the bainitic transformation, which include some important research results and key controversial points,i.e., bainite definition, incomplete phenomenon, solute-drag and solute drag-like effects,the shape, characteristics,nature of the surface relief,crystallography,initial carbon content in bainitic ferrite, the so-called midrib of bainite, source and formation model of lower bainitic carbide,etc., were briefly reviewed.Correspondent: WANG Jiajun, Department of Materials Science and Engineering,(Tsinghua University,Beijing 100084)
|
|
Received: 18 November 1994
|
| 1RobertsonJM.JISI,1929;119:3912 DavenportES,BainEC.TransAIME,1930;90:1173方鸿生,王家军.金属热处理学报,1994;15(4):待发表4 Ko T,CottrellSA.JISI,1952;172:3075 KoT.JISI,1953;175:166ChristianJW.DecompositionAustenitebyDiffusionalProcesses.NY:IntersciencePublishers,1962:3717OblackJM,HehemannRF.Transformations&HardenabilityinSteels,AnnArbor,MI:ClimaxMolybdenumCompany,1967:158HehemannRF,TrioanoAR.MetProg,1956;70(2):979HehemannRF.In:AaronsonHIed.,PhaseTransformations.MetalsPark,OH:ASM,1970:39710BhadeshiaHKDH,EdmondsDV.Metall Trans,1979:10A:89511康沫狂.西北工业大学学报,1990;增刊:112俞德刚.合金中温相变学说的发展及其分歧,上海交通大学科技交流室,198913冯华,康沫狂,李春信.第一届全国贝氏体相变会议论文集,1987,广东,惠州14BhadeshiaHKDH,EdmondsDV.ActaMetall,1980;28:126515EntiwRI.In:ZackayVF.AaronsonHIeds.,DecompositionofAustenitebyDiffusionProcesses.NY:Intersciencepublishers,1962:29516HillertM.In:ZackayVF,AaronsonHIeds.,DecompositionofAustenitebyDiffusionalProcesses.IntersciencePublishers,NY:IntersciencePublishers,1962:19717俞德刚,陈大军,郑经弘.贝氏体铁素体的相变基元和贝氏体θ碳化物的来源及相变的表面浮雕,上海交通大学材料系,1988:418AaronsonHI.In:ZackayVF,AaronsonH I,eds.,DecompositionofAustenitebyDiffusionalPro-cesses,NY:IntersciencePublishers,1962:38719RigsbeeJM,AaronsonHI.ActaMetall,1979;27:35120徐启昆,康戈文.重庆大学学报,1993;16(3):5921方鸿生,王家军.兵器材料科学与工程,1994;17(2):322HuangD,ThomasG.MetallTrans,1972;3A:34323PickeringFB.MetallTrans,1977;8A:10924KaufmanL,RacliffeL,CohenM.In:ZackayVF,AaronsonHLeds.,DecompositionofAustenitebyDiffusionalProcesses.NY:IntersciencePublishers,1962:31325杨柳.清华大学博士学位论文,198826 PurdyGR,HillertM.ActaMetall.1984,32:82327 Hehemann R F,Kinsman K R,AaronsonHI.MetallTrans,1972;3A:107728RigsbeeJM,MennonE SK,LeeHJ,AaronsonHI.ScrMetall,1983;17:146129 BhadeshiaHKDH,ScrMetall,1983;17:147530 BhadeshiaHKDH.ScrMetall.1987;21:101731BhadeshiaHKDH.ChristianJW.MetallTransA,1990;21A:76732AaronsonHI,ReynoldsWT.Jr,ShifletGJ,SpanosG.MetallTrans,1990;21A:134333 ShifletGJ,AaronsonHI.MetallTrans,199o;21A:141334 ReynoldsWT.Jr,LiFZ,ChuiCK,ArronsonHI,MetallTrans,1990;21A:143335LeeHJ,SpanosG,ShifletGJ,AaronsonHI.ActaMetall,1988;36:112936AaronsonHI.TheMechanismofPhaseTransformationsinCrystallineSolids.London:InstituteofMetals,1969;27037康沫狂,胡光立,谭若兵.西北工业大学学报,1990;增刊:3438 WechslerMS,LiebermanDS,ReadTA.Trans AIME,1953;194:150339BowlesJS,MackenieJK.ActaMetall,1954;2:12940BilbyBA,ChristianJW.TheMechanismof PhaseTransformationsinMetals.London:InstituteofMetals,1956:12141 CornelisI,WaymanCM.ActaMetall,1974;22:30142 SmithS,BowlesJS.ActaMetall,1960;8:40543GoldensteinH,AaronsonHI.MetallTrans,1990;21A:146544WeverF,MathieuK,MittKW.InstEnsenforsch,1940;22:945LymanT,TroianoAR.Trans ASM,1946;37:40246BoswellPG,KinsmanKR,ShifletGJ,AaronsonHI.MechanicalPropertiesandPhaseTransfor-mationsinEngineeringMaterials.Warrendale,PA:TSM-AIME,1986:44547AaronsonHI.In:AaronsonHIed.,PhaseTransformations.MetalsPark,OH:ASM,1970:31348ReynoldsWT.Jr,Brenner SS,ArronsonHI.ScrTrans.,1988;22:134349杨柳,方鸿生,孟至和.金属学报,1992;28:A1650ReynoldsWT.Jr,LiuSK,LiFZ,HartfieldS,ArronsonHI.MetallTrans,1990,21A:147951BradleyJR,AaronsonHI.MetallTrans,1981,12:172952LiuSK,ReynoldsWTReynoldsJr,HuH,ShifletGJ,AaronsonHI.MetallTrans,1985;16A:45753ClarkHM,WaymanCM.PhaseTransformations.MetalsPark,OH:ASM,1970:5954AaronsonHI.ScrMetall,1980;14:82555LeeHJ,AaronsonHI.AclaMetall,1988;36:78756DahmenU.ScrMetall,1987,21:102757BhadeshiaHKDH.ScrMetall,1980;14:82158 BhadeshiaHKDH.ActaMetall,1981;29:111759ChristianJW,EdmondsDV.ProcInterConfonPhaseTransformationsinFerrousAlloys,Warrendale,PA:TSM-AIME,1983:29360LairdC,Aaronson,HI.ActaMetall,1967;15:7361LiuYC,AaronsonHI.ActaMetall,1970;18:84562KinsmanKR,EichenE,AaronsonHI.MetallTrans.1975;6A:30363 PitschW.ArchEisenhuettenw,1963;34,38164PickeringFB.Transformation&Hardenabilityinsteels.AnnArbor,MI:ClimaxMolybdenumCompany,1967:10965BhadeshiaHKDH.ActaMetall,1980;28:110366ShackletonDN,KellyPM.PhysicalPropertiesofMartensite&Bainite,Specialreport,ISI,1965;93:12667WellsMGH.ActaMetall,1964;12:38968AaronsonHI,PlichtaMR,FrantiGW,RussellKC.MetallTrans,1978;9A:36369OkaM,OkamotoH,IshidaK.MetallTrans,1990;21A:84570SrinivasanGR,WaymanCM.ActaMetall,1968;16:60971SandvikBPJ,WaymanCM.MetallTrans,1983;14A:82372AaronsonH I,LeeHJ.ScrMetall,1987;21:101173BhadeshiaHKDH,WaughAR.ActaMetall,1982;30:77574KinsmanKR,EichenE,AaronsonHI.MetallTrans,1971;2A(1):34675刘文西,邹美运,马福本,金属学报,1982;17:13776GreningerAB,TroianoAR.TransAIME,1940;140:30777 SchaaberO.TransAIME,1955;203:55978KennonNF,EdwardsRH.J AustInst.Metals,1970;15:19579OkamotoH,OkaM.MetallTrans,1985;16A:225780OkamotoH.MetallTrans,1986;17A:111381BilbyBA,ChristianJW.JISI,1961;197:12282GreningerAB,TroianoAR.TransAIME,1949;185:59183徐祖耀.马氏体相变与马氏体,北京:科学出版社,1980:10784WasilewskiRJ.MetallTrans,1970;1A:264185SpanosG,FangHS,SarmaDS,AaronsonHI.MetallTrans,1990;21A:139186LaiGY.MetallTrans,1975;6A:146987FangHS,WangJJ,ZhengYK.MetallTrans,1994;25(9),inpublishing88JinQ,FangHS.MetallTrans,1990;21A:263789王家军,清华大学博士学位论文,199390HoneycombeRWK,In:MarderAR,GoldsteinJIeds.,ProceedingofanInternationalConferenceonPhaseTransformationsinFerrousAlloys,Warrendale,PA:TSM-AIME,1983;25991方鸿生,王家军.金属学报,1994;30:491l |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|