| MICROSTRUCTURES OF Mg-Zr, Mg-Zn AND Mg-Zn-Zr ALLOYS |
| LUO Zhiping;ZHANG Shaoqing Institute of Aeronautical Materials; Beijing; China doctoral candidate;P.O. Box 81-4; Beijing 100095;China |
|
Cite this article:
LUO Zhiping;ZHANG Shaoqing Institute of Aeronautical Materials; Beijing; China doctoral candidate;P.O. Box 81-4; Beijing 100095;China. MICROSTRUCTURES OF Mg-Zr, Mg-Zn AND Mg-Zn-Zr ALLOYS. Acta Metall Sin, 1993, 29(4): 30-36.
|
|
|
Abstract Microstructural studies have been made on the Mg-0.54Zr, Mg-5.68Zn andMg-5.65Zn-0.50Zr alloys in the as-cast and homogenenized states. The lenticular plates of{012} twins were found in the three alloys. After homogenization, the ZrH_2 phase formed inthe Mg-0.54Zr alloy. The Mg_7Zn_8 phase of cubic structure with α=1.417 nm distributes atthe grain boundaries of Mg-5.68Zn alloy. After homogenization, the Mg_7Zn_8 phase dissolvesand the MgZn_2 phase occurs. The as-cast Mg-5.65Zn-0.50Zr alloy consists ofMgZn_2 phase and Zn-Zr compounds. After homogenization, the dispersed acicularMgZn_2 phase may precipitate.
|
|
Received: 18 April 1993
|
1 北京航空材料研究所.航空材料学.上海:上海科学技术出版社,1985:192 2 Emley E F. Principles of Magnesium Technology. Oxford: Pergamon Press, 1966: 249 3 Портной К И,Лебедев АА 著,林裴译.镁合金手册.北京:冶金工业出版社,1959: 77 4 张少卿,鲁立奇,余应梅.航空材料,1982,2(1) :13 5 张少卿,金属学报,1989;25:A346 6 黄孝瑛.电子显微镜图像分析原理与应用.北京:宇航出版社,1989:171 7 Clark J B. Acta Metall, 1965, 13: 1281 8 Joint Committee on Powder Diffraction Standards. PDF No. 8--269, Powder Diffraction File Inorganic Phases. Pennsylvania: JCPDS, 1983 9 Лашко Н Ф等著.金钦乾,徐澄宇,马翔译.钢和合金的物理-化学相分析.北京:国防工业出版社,1982:273 10 Hanson M. Constitution of Binary Alloys. New York: McGraw-Hill, 1958: 929 11 Raynor G V. The Physical Metallurgy of Magnesium and Its Alloys. London: Pergamon Press, 1959: 200--202w |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|