THERMODYNAMIC CALCULATION OF Fe-P-j SYSTEM MELT
DING Xueyong;WANG Wenzhong;HAN Qiyong Northeastern University University of Science and Technology Beijing
Cite this article: 

DING Xueyong;WANG Wenzhong;HAN Qiyong Northeastern University University of Science and Technology Beijing. THERMODYNAMIC CALCULATION OF Fe-P-j SYSTEM MELT. Acta Metall Sin, 1993, 29(12): 21-26.

Download:  PDF(290KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The activity interaction parameters between alloying elements and P in liquidFe at 1873K were obtained by the thermodynamic calculation. The calculated values arebasically accordant with experimental ones.
Key words:  Fe-P-j melts      activity interaction parameter      thermodynamic calculation     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I12/21

1 Ichise E, Moro-oka A, Trans Iron Steel Inst Jpn, 1988; 28: 153
2 The 19th Committee on Steelmaking, The Japan Society for the Promotion of Science. Steelmaking Data Sourcebook. Gordon and Bresch Science Publishers, 1988: 280
3 张圣弼,李道子.相图--原理、计算及在冶金中的应用.北京:冶金工业出版社,1986:446
4 Toop G W. Trans Metall Soc AIME, 1965; 233. 850
5 Miedema A R, De Chatel P F, De Boer F R. Physica, 1980; 100B: 1
6 丁学勇.北京科技大学博士学位论文,1992
7 Niessen A K, De Boer F R, Boom R, De Chatel P F, Mattens W C M, Miedema A R. Calphad, 1983; 7. 51?
[1] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[2] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[3] YU Jiaying, WANG Hua, ZHENG Weisen, HE Yanlin, WU Yurui, LI Lin. Effect of the Interface Microstructure of Hot-Dip Galvanizing High-Strength Automobile Steel on Its Tensile Fracture Behaviors[J]. 金属学报, 2020, 56(6): 863-873.
[4] Yu HUANG, Guoguang CHENG, You XIE. Modification Mechanism of Cerium on the Inclusions in Drill Steel[J]. 金属学报, 2018, 54(9): 1253-1261.
[5] HAN Guomin, HAN Zhiqiang, Alan A. Luo, Anil K. Sachdev, LIU Baicheng. PHASE FIELD SIMULATION ON MORPHOLOGY OF CONTINUOUS PRECIPITATE Mg17Al12IN Mg-Al ALLOY[J]. 金属学报, 2013, 49(3): 277-283.
[6] LIANG Jingjing, ZHU Ming, YUAN Zhonghua, WANG Junwu, JIN Tao,SUN Xiaofeng, HU Zhuangqi. INFLUENCE OF Re ON THE PHASE CONSTITUENT OF A NiCoCrAlY COATING ALLOY[J]. 金属学报, 2013, 49(3): 330-340.
[7] MA Yue SU Hang PAN Tao YU Yinhong YANG Caifu ZHANG Yongquan PENG Yun. STUDY OF COMPLEX DUCTILE INCLUSIONS CONTROLLING IN MEDIUM-HIGH CARBON STEELS[J]. 金属学报, 2012, 48(11): 1321-1328.
[8] WANG Yi SUN Feng DONG Xianping ZHANG Lanting SHAN Aidang. THERMODYNAMIC STUDY ON EQUILIBRIUM PRECIPITATION PHASES IN A NOVEL Ni-Co BASE SUPERALLOY[J]. 金属学报, 2010, 46(3): 334-339.
[9] Chun-guang Kuai; Zhifang Peng. ELEMENTAL PARTITIONING CHARACTERISTICS AND STABILITY OF EQUILIBRIUM PHASES DURING 450-1200℃ IN T/P91 HEAT-RESISTANT STEEL[J]. 金属学报, 2008, 44(8): 897-900 .
[10] ;. RESEARCH ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF A NEW WROUGHT SUPERALLOY[J]. 金属学报, 2008, 44(5): 540-546 .
[11] LUO Lihua; DING Xueyong; GUO Dan; CAO Wenbin; ZOU Zongshu; WANG Wenzhong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)( University of Science and Technology Beijing; Beijing 1100083). DATABASE SOFTWARE DEVELOPMENT FOR ACTIVITY AND INTERACTION MRAMETER OF ALLOY SYSTEMS[J]. 金属学报, 1998, 34(4): 388-392.
[12] DING Xueyong;WANG Wenzhong(Northeastern University;Shenyang). A NEW THERMODYNAMIC CALCULATION FORMULA FOR ACTIVITY OF COMPONENT IN BINARY SYSTEM[J]. 金属学报, 1994, 30(22): 444-447.
[13] G Xueyong(Northeastern University;Shenyang);FAN Peng;HAN Qiyong(University of Science and Technology Beijing)(Manuscript received 8 April;1993;in revised form 15 July;1993). MODELS OF ACTIVITY AND ACTIVITY INTERACTION PARAMETER IN TERNARY METALLIC MELT[J]. 金属学报, 1994, 30(14): 49-60.
No Suggested Reading articles found!