MATHEMATICAL MODELLING OF RACEWAY IN BLAST FURNACE
CHEN Yisheng;HE Youduo Baotou University of Iron and Steel Technology
Cite this article: 

CHEN Yisheng;HE Youduo Baotou University of Iron and Steel Technology. MATHEMATICAL MODELLING OF RACEWAY IN BLAST FURNACE. Acta Metall Sin, 1993, 29(10): 51-56.

Download:  PDF(428KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A mathematical model to represent the fluid flow, temperature distributionand mass transfer in raceway of blast furnace has been developed. The model is used for pre-dicting the velocity, temperature, and concentration field of raceway in different operationconditions of blast furnace. Results contribute to the understanding of the transport processinvolved in such a system. The model can also be used for optimising the blast furnace opera-tions and the calculation of combustion of pulverized coal.
Key words:  raceway      blast furnace      velocety field      temperature field      concentration field     
Received:  18 October 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I10/51

1 Wagstaff J B, Holman W H. J Met, 1952; 4: 709
2 中村正和,杉山乔,鹈野健夫,原行明,近藤真一.铁钢,1977;63:28
3 稻谷稔宏,福武刚,滨田尚夫,近藤幹夫,冈部侠儿.铁钢,1976;62:25
4 羽田野道春,平冈文章,福田充一朗,增池保.铁钢,1976;62:505
5 成兰伯,曾祥明.钢铁,1982;17:54
6 Kase M, Sugata M, Yamaguchi K, Nakagome K. Trans Iron Steel Inst Jpn, 1982; 22. 811
7 Hillnhuter F W, Kister H, Kruger B. Ironmaking Proc, 1975; 34: 368
8 桑原守,谢裕生,鞭岩.铁钢,1980;66:1918
9 福武刚著,杜鹤桂译.高炉回旋区和炉缸工作文集,北京:冶金工业出版社,1986
10 Jamaluddin A S, Wall T F, Truelove J S. Ironmaking Steelmaking, 1986; 13: 91
11 桑原守,赫冀成,鞭岩.铁钢,1986;72:1847
12 王应时,范维澄,周力行,徐旭常.燃烧过程数值计算,北京:科学出版社,1986
13 谢裕生,车秀珍,李琪.钢铁,1985;20(10) :12
[1] TANG Haiyan, LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan. Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control[J]. 金属学报, 2020, 56(12): 1629-1642.
[2] Xinhua LIU, Huadong FU, Xingqun HE, Xintong FU, Yanqing JIANG, Jianxin XIE. Numerical Simulation Analysis of Continuous Casting Cladding Forming for Cu-Al Composites[J]. 金属学报, 2018, 54(3): 470-484.
[3] Xiaoyu CHONG, Guangchi WANG, Jun DU, Yehua JIANG, Jing FENG. Numerical Simulation of Temperature Field and Thermal Stress in ZTAp/HCCI Composites DuringSolidification Process[J]. 金属学报, 2018, 54(2): 314-324.
[4] Yadong CHEN, Yunrong ZHENG, Qiang FENG. EVALUATING SERVICE TEMPERATURE FIELD OF HIGH PRESSURE TURBINE BLADES MADE OF DIRECTIONALLY SOLIDIFIED DZ125 SUPERALLOY BASED ON MICRO-STRUCTURAL EVOLUTION[J]. 金属学报, 2016, 52(12): 1545-1556.
[5] ZHAO Bo, WU Chuansong,JIA Chuanbao, YUAN Xin. NUMERICAL ANALYSIS OF THE WELD BEAD PROFILES IN UNDERWATER WET FLUX-CORED ARC WELDING[J]. 金属学报, 2013, 49(7): 797-803.
[6] XU Qingdong, LIN Xin, SONG Menghua, YANG Haiou, HUANG Weidong. MICROSTRUCTURE OF HEAT-AFFECTED ZONE OF LASER FORMING REPAIRED 2Cr13 STAINLESS STEEL[J]. 金属学报, 2013, 49(5): 605-613.
[7] PANG Ruipeng, WANG Fuming, ZHANG Guoqing, LI Changrong. STUDY OF SOLIDIFICATION THERMAL PARAMETERS OF 430 FERRITE STAINLESS STEEL BASED ON 3D-CAFE METHOD[J]. 金属学报, 2013, 49(10): 1234-1242.
[8] KE Changbo, CAO Shanshan, MA Xiao, HUANG Ping, ZHANG Xinping. PHASE FIELD SIMULATION OF AUTO-CATALYTIC GROWTH EFFECT OF COHERENT Ni4Ti3 PRECIPITATE IN NiTi SHAPE MEMORY ALLOY[J]. 金属学报, 2013, 49(1): 115-122.
[9] WEI Jie DONG Junhua KE Wei. NUMERICAL SIMULATION AND EXPERIMENTAL STUDY ON TEMPERATURE FIELD DURING CHEMICAL REAGENT COOLING PROCESS OF HOT ROLLED REBAR[J]. 金属学报, 2012, 48(1): 115-121.
[10] FENG Mingjie WANG Engang HE Jicheng. NUMERICAL SIMULATION ON TEMPERATURE FIELD IN HIGH SPEED STEEL COMPOSITE ROLL DURING CONTINUOUS POURING PROCESS FOR CLADING I. Graphite Mould Method[J]. 金属学报, 2011, 47(12): 1495-1502.
[11] FENG Mingjie WANG Engang HE Jicheng. NUMERICAL SIMULATION ON TEMPERATURE FIELD IN HIGH SPEED STEEL COMPOSITE ROLL DURING CONTINUOUS POURING PROCESS FOR CLADDING
II. Copper Mould Method
[J]. 金属学报, 2011, 47(12): 1503-1512.
[12] LI Baokuan DAI Fengyu QI Fengsheng YANG Ran. FLOW FIELD AND CONCENTRATION FIELD OF ALLOYING ADDITION IN CLAD STEEL CONTINUOUS CASTING MOLD USING LONG AND SHORT NOZZLES[J]. 金属学报, 2010, 46(6): 736-742.
[13] YU Haiqi ZHU Miaoyong. 3-D NUMERICAL SIMULATION OF FLOW FIELD AND TEMPERATURE FIELD IN A ROUND BILLET CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC STIRRING[J]. 金属学报, 2008, 44(12): 1465-1473.
[14] Qiaodan Hu; Peng Luo; Jianguo Li. FINITE ELEMENT MODELING OF TEMPERATURE DISTRIBUTION IN FIELD ACTIVATED SINTERING OF MoSi2-SiC COMPOSITE[J]. 金属学报, 2008, 44(10): 1253-1259 .
[15] . Numerical Simulation of two-phase Solidification Process of[J]. 金属学报, 2007, 43(6): 668-672 .
No Suggested Reading articles found!