Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (10): 46-50    DOI:
Current Issue | Archive | Adv Search |
GROWTH OF HOT CRACKS IN LIQUID-FORGED STEEL FLAT FLANGES
LUO Shoujing;HU Lianxi;HUO Wencan Harbin Institute of Technology
Cite this article: 

LUO Shoujing;HU Lianxi;HUO Wencan Harbin Institute of Technology. GROWTH OF HOT CRACKS IN LIQUID-FORGED STEEL FLAT FLANGES. Acta Metall Sin, 1993, 29(10): 46-50.

Download:  PDF(1757KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The morphology and feature of hot cracks in liquid forged steel flat frangeshave been observed. Once the cracks occur, they will propagate throguh 4 stages, and revealthemselves obviously as 4 featured zones. The growth of the hot cracks seems to be depen-dent upon certain technological factors, such as: liquid steel quality, solidification and stressedstate on workpieces, etc.
Key words:  liquid forging      steel flat flange      hot crack     
Received:  18 October 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I10/46

1. 孙宗玉,罗守靖,彭其凤.山东机械,1984;(3) :13
2. 罗守靖,霍文灿,胡连喜.钢铁,1991;(8) :54
[1] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[2] Yaohong LIU,Zhaohui WANG,Ke LIU,Shubo LI,Wenbo DU. Effects of Er on Hot Cracking Susceptibility of Mg-5Zn-xEr Magnesium Alloys[J]. 金属学报, 2019, 55(3): 389-398.
[3] Yingkai SHAO, Yuxi WANG, Zhibin YANG, Chunyuan SHI. Plasma-MIG Hybrid Welding Hot Cracking Susceptibility of 7075 Aluminum Alloy Based on Optimum of Weld Penetration[J]. 金属学报, 2018, 54(4): 547-556.
[4] Feng WANG,Haikuo DONG,Zhi WANG,Pingli MAO,Zheng LIU. Hot Cracking Behavior of Mg-5Al-xCa Alloys[J]. 金属学报, 2017, 53(2): 211-219.
[5] Kejian LI,Zhipeng CAI,Yifei LI,Jiluan PAN. EVOLUTION BEHAVIOR OF LAVES PHASE IN FB2 MARTENSITIC STAINLESS STEEL DURING WELDING[J]. 金属学报, 2016, 52(6): 641-648.
[6] LI Haoyu, BAI Yuanyuan, ZHANG Haitao, WU Xin, ZHANG Zhiqiang, LE Qichi. EFFECT OF Mn ON HOT CRACKING TENDENCY OF Mg-6.5Zn ALLOYS[J]. 金属学报, 2014, 50(10): 1237-1243.
[7] DING Hao(Xi'an Jiaotong University; Xi'an 710049); FU Hengzhi;LIU Zhonguan (Northwestern Polytechnical University. Xi'an 710072); CHEN Rongzhang; LIUBocao;ZHONG Zhengung;TANG Dingzhong(Beijing Institute of Aeronautical Materials; Beijing 100095). COMPENSATION OF SOLIDIFICATION CONTRACTION AND HOT CRACKING TENDENCY OF ALLOYS[J]. 金属学报, 1997, 33(9): 921-926.
[8] DING Hao;FU Hengzhi;LUO Shuanzhu;LIU Zhongyuan;ZHANG Kefu(Northwestern Polytechnical University;Xi'an 710072). INFLUENCE OF COMPOSITION ON HOT CRACKING TENDENCY OF DIRECTIONALLY SOLIDIFIED Al-Cu ALLOY[J]. 金属学报, 1995, 31(8): 376-380.
No Suggested Reading articles found!