| EFFECT OF OXIDE LAYER THICKNESS OVER AI AND AI ALLOY POWDERS ON QUALITY OF THEIR EXPLOSIVE COMPACTS |
| ZHANG Dengxia; MA Chenghui; CAI Ming (Institute of Mechanics; Academia Sinica; Beijing); AI Baoren; ZHANG Jinyuan; ZHU Ruizhen; LIU Chunlan (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
|
Cite this article:
ZHANG Dengxia; MA Chenghui; CAI Ming (Institute of Mechanics; Academia Sinica; Beijing); AI Baoren; ZHANG Jinyuan; ZHU Ruizhen; LIU Chunlan (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). EFFECT OF OXIDE LAYER THICKNESS OVER AI AND AI ALLOY POWDERS ON QUALITY OF THEIR EXPLOSIVE COMPACTS. Acta Metall Sin, 1992, 28(7): 74-77.
|
|
|
Abstract Observations of microstructure of explosive compacts made of Al or Al-Li alloy powders by atomization with water, nitrogen or ultrasonic Ar gas were carried out under optical and scanning electron microscopes. The results indicate that super quality explosive compact can only be obtained by powders of which the thickness of the exide lager is less than 30 nm.
|
|
Received: 18 July 1992
|
| 1 Filnn J E, Williamson R L, Berrg R A, Wrigat R N, Gupta Y M, Williams M. J Appl Phys, 1988; 64: 1446 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|