| EFFECT OF SLIP ORIENTATION ON STRESS RESPONSE, INTERNAL FRICTION AND ULTRASONIC ATTENUATION DURING CYCLIC DEFORMATION IN Al SINGLE CRYSTALS |
| XIA Yuebo;ZHANG Tianyi;FEI Guangtao;ZHOU Xing State Key Laboratory for Fatigue and Failure of Materials; Institute of Metal Research; Academia Sinica; Shenyang Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; Academia Sinica; Hefei Correspondent associate professor; Insttitute of Metal Research; Academia Sinica; Shenyang 110015 |
|
Cite this article:
XIA Yuebo;ZHANG Tianyi;FEI Guangtao;ZHOU Xing State Key Laboratory for Fatigue and Failure of Materials; Institute of Metal Research; Academia Sinica; Shenyang Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; Academia Sinica; Hefei Correspondent associate professor; Insttitute of Metal Research; Academia Sinica; Shenyang 110015. EFFECT OF SLIP ORIENTATION ON STRESS RESPONSE, INTERNAL FRICTION AND ULTRASONIC ATTENUATION DURING CYCLIC DEFORMATION IN Al SINGLE CRYSTALS. Acta Metall Sin, 1992, 28(6): 33-39.
|
|
|
Abstract Studies were made of the variation of stress response, σ, internal friction, Q~(-1), and ultrasonic attenuation Aa, during cyclic deforamtion and correlation among them withdifferent slip orientation Al single crystals. Results indicate that they have obvious depen-dence upon slip orientation of Al single crystals. They are many differences for Q~(-1), △αand σbetween mono-slip and multi-slip Al single crystals. For the Al single crystals with sameorientation, the increase of σ corresponds with reduction of Q~(-1) and increase of △α, yet therequired number of cycles approaching the maximum of △α may be less than that of α up tomaximmu. And the Q~(-1) and σ may reach minimum and maximum, respectively, at samenumber of cycle.
|
|
Received: 18 June 1992
|
1 Alden T. H, Backofen W A. Acta Metall, 1961; 9: 352 2 Xia Y. B., Wang Z. G. Wang R H, Phys Status Solidi, 1990; 120a 125 3 Liu Wei, Wang Zhongguang, Xia Yuebo, Phys Status Solidi, 1989 114a: 177 4 朱震刚,周星,费广涛,仪器仪表学报,1988;9:396 5 Nowick A S, Berry B S. Anelastic Reiaxation in Crystaline Solids. New York: Academic Press, 1972: 22, 26 6 Mnghrabi H. Mater Sci Eng, 1978; 33: 207 7 费广涛,中国科学院固体物研究所硕士学位论文,1991 8 Granato A, Luecke K. J Applphys, 1856; 27: 583{ |