ACTIVITY OF TiO_2 IN MOLTEN BLAST FURNACE SLAG CONTAINING TITANIUM OXIDE
LIU Huanming;DU Hong;YANG Zupan;LI Guodong;DU Kun Benxi Iron and Steel Company; Northeast University of Technology; Shenyang; Centrel Iron and Steel Research Institute; Ministry of Metallurgical Industry. Beijing
Cite this article: 

LIU Huanming;DU Hong;YANG Zupan;LI Guodong;DU Kun Benxi Iron and Steel Company; Northeast University of Technology; Shenyang; Centrel Iron and Steel Research Institute; Ministry of Metallurgical Industry. Beijing. ACTIVITY OF TiO_2 IN MOLTEN BLAST FURNACE SLAG CONTAINING TITANIUM OXIDE. Acta Metall Sin, 1992, 28(2): 47-51.

Download:  PDF(421KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Activity of TiO_2 in the molten blast furnaee slag containing titanium oxide has been examined at 1500℃ by means of "molten slag-Sn" chemical equilibrium method, using metallic Sn as flux and graphite as deoxidizer, together with phase diagram calculation. In the pentary slag sys-tem CaO--MgO--SiO_2--TiO_2--Al_2O_3, a_(TiO_2)=0.01--0.05 or 0.02--0.10 with pure liquid or solid TiO_2 as normal state, respectively. The activity and activity coefficient of TiO_2 in relation to concen-tration of titanium oxide have been discussed.
Key words:  titanium oxide      activity      blast furnace      molten slag     
Received:  18 February 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I2/47

1 戚大光,李道昭,张桂欣,樊钟曾.钢铁钒钛,1984;2:79
2 邹元燨,赵彭年,曹兆民.金属学报,1963;6:121
3 王常珍,杨代银.金属学报,1979;15:433
4 陈崇禧,赵文祥.金属学报,1983;19:A1
5 刘焕明,杨祖磐,田彦文.金属学报,1989;25:B293
6 Hillert L. Acta Chem Scand, 1965; 19: 1516
7 董希琳.中国科学院化工冶金研究所硕士学位论文,1986
8 伊藤公久,佐野信雄.铁钢,1981;67:2131
9 Turkdogan E T. Physical Chemistry of High Temperature Technology. New York, 1980: 5--26
10 Aylward G H,Findlay T J V编,周宁怀译.SI化学数据表.北京:高等教育出版社,1985:64,
[1] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[2] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[3] Xiaofeng LU, Ming XIAO, Yangmei CHEN, Bangcheng YANG. Bioactivity of Titanium Metal Hybridized with Inactivated Bacterial Biofilm[J]. 金属学报, 2017, 53(10): 1402-1412.
[4] Muqin LI, Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG. The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. 金属学报, 2017, 53(10): 1337-1346.
[5] Chuan HONG,Yunming GAO,Chuanghuang YANG,Zhibo TONG. ELECTROCHEMICAL BEHAVIOR OF Ni2+ IN SiO2-CaO-MgO-Al2O3 MOLTEN SLAG AT 1673 K[J]. 金属学报, 2015, 51(8): 1001-1009.
[6] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[7] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[8] WU Ling. The improvement of regular solution model based on GA-NN and its application in binary slag system[J]. 金属学报, 2008, 44(7): 799-802 .
[9] Yuan Liu. Improvement of Calculation Method for the Activity Coefficient of Multi-component Alloys[J]. 金属学报, 2007, 43(5): 503-508 .
[10] LE Qichi; CUI Jianzhong. Thermodynamics Properties of Ternary Bath of Coloring Hot--Dip Galvanization[J]. 金属学报, 2006, 42(11): 1182-1186 .
[11] GAO Chuanhou; ZHOU Zhimin; SHAO Zhijiang. Chaotic Local--Region Linear Prediction Of Silicon Content In Hot Metal Of Blast Furnace[J]. 金属学报, 2005, 41(4): 433-436 .
[12] MA Zhongting; J. OHSER; D. JANKE(The Institute of Iron and Steel Technology; Freiberg University of Mining and Technology; Freiberg; Germany). THERMODYNAMIC DESCRIPTION OF MULTICOMPONENT SYSTEMS BY INTERACTION MRAMETERS[J]. 金属学报, 1998, 34(7): 753-762.
[13] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[14] LUO Lihua; DING Xueyong; GUO Dan; CAO Wenbin; ZOU Zongshu; WANG Wenzhong (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)( University of Science and Technology Beijing; Beijing 1100083). DATABASE SOFTWARE DEVELOPMENT FOR ACTIVITY AND INTERACTION MRAMETER OF ALLOY SYSTEMS[J]. 金属学报, 1998, 34(4): 388-392.
[15] ZHANG Ziqing(Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). DISCUSSION ON THE METHOD TO DETERMINE THE ACTIVITY IN SLAGS BY MEANS OF THE SLAGMETAL EQUILIBRIA IN A LIQUID STATE[J]. 金属学报, 1998, 34(3): 299-304.
No Suggested Reading articles found!