Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (4): 59-63    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF HIGH TEMPERATURE REPRESSING ON P SEGREGATION IN 93W-4.5Ni-2.5Fe ALLOY
LI Zhi;XI Jukui;YANG Yunlin Luoyang Institute of Technology
Cite this article: 

LI Zhi;XI Jukui;YANG Yunlin Luoyang Institute of Technology. INFLUENCE OF HIGH TEMPERATURE REPRESSING ON P SEGREGATION IN 93W-4.5Ni-2.5Fe ALLOY. Acta Metall Sin, 1991, 27(4): 59-63.

Download:  PDF(1115KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of high temperature repressing on the P segregation in93W-4.5Ni-2.5Fe alloy has been examined by Auger spectroscopy, EPMA, TEM andSEM. The P was observed to segregate along the W-W interface, especially the W-matrix boundaries, in specimens aged at 1200--1500℃, F.C., but it will be no moreafter repressed. The dislocations in the matrix of as-repressed alloy seem to be influ-ential directly on the segregation of P onio interface. The mechanical propertiesmay decrease with the interfacial segregation of P in the annealed specimens.
Key words:  W-Ni-Fe alloy      high temperature repressing      interface      P segregation      dislocation     
Received:  18 April 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I4/59

1 Lea C, Muddle B C, Edmonds D V. Metall Trans, 1983; 14A: 667--677
2 Rdmonds D V, Jones P N. Metall Trans, 1979; 10A: 289--295
3 胡赓祥,钱苗根.金属学.上海:上海科学出版社,1980:230-233
4 Yodogawa M. Mater Sci Monogr, 1982; 14: 519--525
5 葛昌纯,夏元洛.粉末冶金技术,1984;2(1) :7-14
[1] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[2] HAN Weizhong, LU Yan, ZHANG Yuheng. Mechanism of Ductile-to-Brittle Transition in Body-Centered-Cubic Metals:A Brief Review[J]. 金属学报, 2023, 59(3): 335-348.
[3] LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng. Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance[J]. 金属学报, 2023, 59(3): 349-370.
[4] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[5] ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang. Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface[J]. 金属学报, 2023, 59(11): 1523-1532.
[6] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[7] TIAN Ni, SHI Xu, LIU Wei, LIU Chuncheng, ZHAO Gang, ZUO Liang. Effect of Pre-Tension on the Fatigue Fracture of Under-Aged 7N01 Aluminum Alloy Plate[J]. 金属学报, 2022, 58(6): 760-770.
[8] GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin. Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy[J]. 金属学报, 2022, 58(6): 746-759.
[9] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[10] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[11] WU Xiaolei, ZHU Yuntian. Heterostructured Metallic Materials: Plastic Deformation and Strain Hardening[J]. 金属学报, 2022, 58(11): 1349-1359.
[12] LU Lei, ZHAO Huaizhi. Progress in Strengthening and Toughening Mechanisms of Heterogeneous Nanostructured Metals[J]. 金属学报, 2022, 58(11): 1360-1370.
[13] HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong. Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram[J]. 金属学报, 2021, 57(9): 1199-1214.
[14] ZHAO Yuhong, JING Jianhui, CHEN Liwen, XU Fanghong, HOU Hua. Current Research Status of Interface of Ceramic-Metal Laminated Composite Material for Armor Protection[J]. 金属学报, 2021, 57(9): 1107-1125.
[15] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
No Suggested Reading articles found!