Abstract From the thermodynamical analysis, the criterion of optimization inheating process of materials with minimum energy consumption, so called optimalheating process criterion, has been established. Based upon the criterion togetherwith the linear quadratic control theory, a new general method for optimizationin heating process was developed. This method is believed to be quite available tosolve the heat supply problems not only in distribution along furnace length butalso in time-variation.
|
|
Received: 18 January 1991
|
1 Misaka Y, Takahashi R, ShinJo A, Nariai Y, Kooriki M. Iron Steel Eng. 1982; 59(5) : 51 2 Schurko R J, Weinstein C, Hanne M K, Pellecchia D J. Iron, Steel Eng. 1987: 64(5) : 37 3 宁宝林,陈海耿,杨泽宽,王英斌.冶金能源,1989;(5) :37 4 谢绪恺.现代控制理论基础,沈阳;辽宁人民出版社,1980:341 5 Hottel H C. J Inst Fuel, 1961; (6) : 220m |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|