Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (2): 142-145    DOI:
Current Issue | Archive | Adv Search |
PHASE DIAGRAMS OF KF-LiCl-BaCl_2 AND LiF-LiCl-BaCl_2 SYSTEMS
YAN Licheng;YANG Jinxiu;ZHU Lei;XU Jingyan;FAN Jinxia Shanghai University of Science and Technology Suzhou Teachers' School Department of Chemistry;Shanghai University of Science and Technology; Shanghai 2018000
Cite this article: 

YAN Licheng;YANG Jinxiu;ZHU Lei;XU Jingyan;FAN Jinxia Shanghai University of Science and Technology Suzhou Teachers' School Department of Chemistry;Shanghai University of Science and Technology; Shanghai 2018000. PHASE DIAGRAMS OF KF-LiCl-BaCl_2 AND LiF-LiCl-BaCl_2 SYSTEMS. Acta Metall Sin, 1990, 26(2): 142-145.

Download:  PDF(237KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phase diagrams of molten salt systems KF-LiCl-BaCl_2 and LiCl-LiF-BaCl_2 have been determined by visual polythermal method. The relationship be-tween the change of cation radius of monovalent fluoride and the areas of primarycrystal region in the phase diagrams was discussed.
Key words:  phase diagram      molten salt system      KF      LiCl      BaCl_2     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/142

1 #12
2 #12
3 阎立诚,杨金秀,朱鹦鹦.高等学校化学学报,1988;9(7) :726
4 Yan L. Proc Second Japan-China Bilateral Confernce on Molten Salt Chimistry and Technology. Yokohama, Japan. 1988: 137
[1] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[2] Yun XUE,Xue YANG,Yongde YAN,Milin ZHANG,Debin JI,Enyu LI,Wei HAN. ELECTROLYSIS EXTRACTION OF NEODYMIUM FROM LiCl-KCl-AlCl3-Nd2O3 MELTS WITHTHE ASSISTANCE OF AlCl3[J]. 金属学报, 2016, 52(7): 883-889.
[3] LIU Hongji, SUN Junjie, JIANG Tao, GUO Shengwu, LIU Yongning, LIN Xin. ROLLING CONTACT FATIGUE BEHAVIOR OF AN ULTRAHIGH CARBON STEEL[J]. 金属学报, 2014, 50(12): 1446-1452.
[4] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[5] ;. EXPERIMENTAL RESEARCH OF PREPARATION OF CaB6 BY MOLTEN SALT ELECTROLYSIS METHOD[J]. 金属学报, 2008, 44(10): 1243-1246 .
[6] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[7] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[8] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
[9] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[10] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[11] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
[12] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[13] YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
[14] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[15] YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.
No Suggested Reading articles found!