Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (2): 146-148    DOI:
Current Issue | Archive | Adv Search |
TRANSFER OF Ti AND Si BETWEEN SLAGS AND MOLTEN Cu UNDER CONSTANT OXYGEN POTENTIAL
XUE Xiangxin;DU Hegui Northeast University of Technology; Shenyang Department of Ferrous Metallurgy;Northeast University of Technology; Shenyang 110006
Cite this article: 

XUE Xiangxin;DU Hegui Northeast University of Technology; Shenyang Department of Ferrous Metallurgy;Northeast University of Technology; Shenyang 110006. TRANSFER OF Ti AND Si BETWEEN SLAGS AND MOLTEN Cu UNDER CONSTANT OXYGEN POTENTIAL. Acta Metall Sin, 1990, 26(2): 146-148.

Download:  PDF(233KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An experimental study has been made of the mass transfer of Ti and Si betweenslags and molten Cu under constant oxygen potential at 1500℃. Apparent mass transfer coeffi-cients of Ti and Si in molten Cu were obtained.
Key words:  Cu-Ti-Si alloy      apparent mass transfer     
Received:  18 February 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I2/146

1 Baxter G P, Lansing J E. J Amer Chem Soc, 1920; 42: 419
2 周继程,邹元爔,赵彭年,李鸿明,张子青.中国金属学会编,中国金属学会1979--1980年优秀论文集,第四分册,北京:冶金工业出版社,1984:83
3 森一美,平沢政(广厶),新贝元,圃中朝夫.铁钢,1985;71:1110
4 薛向欣,杜鹤桂.金属学报,1990;26:B7
[1] XUE Xiangxin;DU Hegui Northeast University of Technology; Shenyang Department of Ferrous Metallurgy;Northeast University of Technology;Shenyang;110006. OXIDATION OF Ti IN MOLTEN Cu UNDER WATERY ATMOSPHERE[J]. 金属学报, 1990, 26(1): 153-154.
No Suggested Reading articles found!