THERMODYNAMIC STUDY OF BAINITIC TRANSFORMATION IN Fe-C ALLOYS
WANG Shidao;YU Degang Lanzhou Railway Institute Shanghai Jiaotong University
Cite this article: 

WANG Shidao;YU Degang Lanzhou Railway Institute Shanghai Jiaotong University. THERMODYNAMIC STUDY OF BAINITIC TRANSFORMATION IN Fe-C ALLOYS. Acta Metall Sin, 1989, 25(4): 23-29.

Download:  PDF(580KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The growth of bainitic ferrite is a couple process of the shear trans-formation of Fe atoms and the diffusion of C atoms. The diffusion growth of fer-rite is impossible when the temperature is below 400℃, and the paraequilibriumshear growth may occur at the temperature below 550℃. This paraequilibrium sheargrowth model explains the overlap of the bainites created from two growth mecha-nisms at 400--550℃.
Key words:  Fe-C alloys      bainite      thermodynamics     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/23

1 Trivedi R. In: Aaroason H I et al. eds., Proc Int Conf on Solid→Solid Phase Transformations, New York: AIME, 1982: 477
2 Hillert M. Metall Trans, 1975; 6A: 5
3 Hultgren A. Jernkontorets Ann. 1951; 135: 403
4 Hillert M.Thermodynamics of Alloys,北京科技大学讲演稿,1980
5 王世道,马氏体相变的能量学理论,兰州铁道学院科学报告,1986;
6 Kaufman L, Radcliff SV, Cohen M. In: Zackay V F, Aaronson H. I eds. Decomposition of austenite by diffusional processes, New York: Interscience 1962: 313
7 Shiflet G J. Bradlly J R, Aaronson H I. Metall Trans, 1978; 9A: 999
8 俞德刚,陈大军,郑经綋,何忆蓉,沈甫法.金属学报,1988;24:A379
[1] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[2] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[3] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[4] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[5] ZHU Dongming, HE Jiangli, SHI Genhao, WANG Qingfeng. Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel[J]. 金属学报, 2022, 58(12): 1581-1588.
[6] JIANG Zhonghua, DU Junyi, WANG Pei, ZHENG Jianneng, LI Dianzhong, LI Yiyi. Mechanism of Improving the Impact Toughness of SA508-3 Steel Used for Nuclear Power by Pre-Transformation of M-A Islands[J]. 金属学报, 2021, 57(7): 891-902.
[7] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[8] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[9] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[10] Shixin XU, Wei YU, Shujia LI, Kun WANG, Qisong SUN. Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure[J]. 金属学报, 2018, 54(8): 1113-1121.
[11] Huidong WU, Goro MIYAMOTO, Zhigang YANG, Chi ZHANG, Hao CHEN, Tadashi FURUHARA. Incomplete Bainite Transformation Accompanied with Cementite Precipitation in Fe-1.5(3.0)%Si-0.4%C Alloys[J]. 金属学报, 2018, 54(3): 367-376.
[12] Xiaofeng HU, Haichang JIANG, Mingjiu ZHAO, Desheng YAN, Shanping LU, Lijian RONG. Microstructure and Mechanical Properties of Welded Joint of a Fe-Cr-Ni-Mo Steel with High-Strength and High-Toughness[J]. 金属学报, 2018, 54(1): 1-10.
[13] Liansheng CHEN, Yue LI, Mingshan ZHANG, Yaqiang TIAN, Xiaoping ZHENG, Yong XU, Shihong ZHANG. Effect of Intercritical Dislocation Multiplication to Mn Partitioning and Microstructure Evolution of Bainite in Low Carbon Steel[J]. 金属学报, 2017, 53(11): 1418-1426.
[14] Xiaolu GUI,Baoxiang ZHANG,Guhui GAO,Ping ZHAO,Bingzhe BAI,Yuqing WENG. FATIGUE BEHAVIOR OF BAINITE/MARTENSITE MULTIPHASE HIGH STRENGTH STEEL TREATEDBY QUENCHING-PARTITIONING-TEMPERING PROCESS[J]. 金属学报, 2016, 52(9): 1036-1044.
[15] Liheng LIU,Chunshan CHE,Gang KONG,Jintang LU,Shuanghong ZHANG. DESTABILIZATION MECHANISM OF Fe-Al INHIBITION LAYER IN Zn-0.2%Al HOT-DIP GALVANIZING COATING AND RELATED THERMODYNAMIC EVALUATION[J]. 金属学报, 2016, 52(5): 614-624.
No Suggested Reading articles found!