Abstract The regular solution model developed by M. Hillert et al is appliedto calculate the driving force of bainitic transformation for Fe-C-Mn ternary alloysin the intermediate temperature range. Focus is made on the thermodynamical dis-cussions for both diffusional and shear mechanisms for bainitic transformations indifferent temperature ranges.
|
Received: 18 April 1989
|
1 Hsu T Y (Xu Zuyao) (徐祖耀), Mou Yiwen (牟翊文). Acta Metall, 1984; 32: 1469 2 Hillert M, Staffanson L I. Acta Chem Scand, 1970; 24: 3618 3 Sharma R C, Purdy Q R, Kirkaldy J S. Metall Trans, 1979; 10A: 1119 4 Ulhrenius B. In: Doane D V, Kirkaldy J S eds., Hardenability Concepts with Application to Steel, AIME, 1978: 28 5 Hsu T Y (Xu Zuyao) (徐祖耀), Chang Hongbing (张鸿冰), Luo Shoufu. J Mater Sci, 1983; 18: 3206 6 Orr R L, Chipman J. Trans. TMS-AIME, 1967; 239: 630 7 赵宇新,李朋兴,徐祖耀.金属学报,1986; 22: A130 8 Himmelblau D M. Applied Nonlinear Programing, New York: McGrow-Hill, Book Company, 1972 9 杨柳.清华大学工学博士论文,1988 10 Heheman R F. Phase Transformation, Metals Park, Ohio: ASM, 1970: 397 11 Coates D E. Metall Trans, 1973; 4A: 2313 12 Hsu T Y (Xu Zuyao) (徐祖耀), Zhang Hongbing (张鸿冰). Acta Metall, 1984; 32: 343 13 Chang Hongbing (张鸿冰), Hsu T Y (Xu Zuyao) (徐祖耀). Acta Metall, 1986; 34: 333t |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|