INTERFACIAL TENSION BETWEEN SLAG AND MATTE
LI Jing;HUANG Kexiong;CHEN Xinmin Central South University of Technology; Changsha
Cite this article: 

LI Jing;HUANG Kexiong;CHEN Xinmin Central South University of Technology; Changsha. INTERFACIAL TENSION BETWEEN SLAG AND MATTE. Acta Metall Sin, 1989, 25(3): 96-101.

Download:  PDF(543KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The interfacial tension between FeO-CaO-SiO-MgO system slag andCu-Fe-S system matte was determinated by the X-ray radiograph sessile drop method.The effects of FeO/SiO ratio in the slag, contents of CaO, FeO, ZnO and CaF_2 inthe slag on interfacial tension and the relation of interfacial tension with the gradeof matte and temperature have been studied. The floatation coefficient and film coef-ficient of slag-matte system has been calculated and the mechanism of the transitionof iron and oxygen from slag to matte has also been discussed.
Key words:  Interfacial tension      matte      slag      sessile drop method     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/96

1#12
2#12
3 Elliott J F, Mounier M. Can Metall Q, 1982: 21: 45
4 黄克雄,李晶,孙铭良,莫鼎成,陈新民.有色金属(冶炼部分),1986;6:31
5 李晶.中南工业大学博士学位论文,1988
6 李晶.中南矿冶学院学报.1984;3:103
7 McKenzie C K. Minto R, Davenport W G. Can Metall Q, 1975; 3: 191
8 李晶,孙铭良,黄克雄.全国第一届有色冶金物理化学年会论文集,中国有色金属学会冶金物化学术委员会,1986:44
9 Tavera F J, Davenport W G. Metall Trans, 1979; 10B: 237
10 Bor F Y, Tarassoff P. Can Metall Q, 1971; 10 (4) : 267
[1] ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang. Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface[J]. 金属学报, 2023, 59(11): 1523-1532.
[2] Qiang WANG, Lianyu WANG, Hongxia LI, Jiawei JIANG, Xiaowei ZHU, Zhancheng GUO, Jicheng HE. Suppression Mechanism and Method of Vortex During Steel Teeming Process in Ladle[J]. 金属学报, 2018, 54(7): 959-968.
[3] Zibing HOU,Jianghai CAO,Yi CHANG,Wei WANG,Han CHEN. Morphology Characteristics of Carbon Segregation in Die Steel Billet by ESR Based on Fractal Dimension[J]. 金属学报, 2017, 53(7): 769-777.
[4] Qing LI,Zixing WANG,Shuyuan XIE. Research on the Development of Mathematical Model of the Whole Process of Electroslag Remelting and the Process Simulation[J]. 金属学报, 2017, 53(4): 494-504.
[5] Chuan HONG,Yunming GAO,Chuanghuang YANG,Zhibo TONG. ELECTROCHEMICAL BEHAVIOR OF Ni2+ IN SiO2-CaO-MgO-Al2O3 MOLTEN SLAG AT 1673 K[J]. 金属学报, 2015, 51(8): 1001-1009.
[6] NI Zifei SUN Yangshan XUE Feng BAI Jing. STUDY ON FABRICATION, MICROSTRUCTURE AND PROPERTIES OF IN SITU TiC PARTICLE ON DISPERSION–STRENGTHENED 304 STAINLESS STEEL[J]. 金属学报, 2010, 46(8): 935-940.
[7] WANG Fang LI Baokuan. ANALYSIS OF ELECTROMAGNETIC FIELD AND JOULE HEATING OF ELECTROSLAG REMELTING PROCESSES[J]. 金属学报, 2010, 46(7): 794-799.
[8] YU Hai-Qi. The interfacial behavior of molten steel and liquid slag in a slab continuous casting mold with electromagnetic brake and argon gas injection[J]. 金属学报, 2008, 44(9): 1141-1148 .
[9] WU Ling. The improvement of regular solution model based on GA-NN and its application in binary slag system[J]. 金属学报, 2008, 44(7): 799-802 .
[10] . Modeling of Three-Phase Flows and Slag Layer Behavior in an Argon Gas Stirred Ladle[J]. 金属学报, 2008, 44(10): 1198-1202 .
[11] Na CAO. Numerical Simulation for the Interfacial Behavior of Steel and Slag in a Slab Continuous Casting Mold with Blowing Argon Gas[J]. 金属学报, 2008, 44(1): 79-84 .
[12] Na CAO. Numerical Simulation for the Interfacial Behavior of Steel and Slag in a Slab Continuous Casting Mold with High Casting Speed[J]. 金属学报, 2007, 43(8): 834-838 .
[13] ZHANG Xiaobing. Thermodynamic Modeling for Controls of Deoxidation and Oxide Inclusions in Molten Steel[J]. 金属学报, 2004, 40(5): 509-514 .
[14] ZHONG Hexiang; WANG Shulan; ZHANG Lijun. Effects of TiC on the Conductivities of Titania Slag[J]. 金属学报, 2004, 40(5): 515-517 .
[15] ZHONG Hexiang; WANG Shulan; ZHANG Lijun. Effects of TiC on the Conductivities of Titania Slag[J]. 金属学报, 2004, 40(5): 515-517 .
No Suggested Reading articles found!