Abstract The mathematical formulas are given for calculating the partial molarthermodynamic properties in a ternary system from its three corresponding binary sys-tems based on the new ternary symmetric model presented by the authors in theforegoing paper. Applying this model to NaCl-BaCl_2-SrCl_2 system, the phase diagramof which as well as some isothermal sections have been calculated. The deviations oftemperature between the calculated and experimental diagrams are less than five de-grees.
|
Received: 18 March 1989
|
1 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists. and 1969, 1975 Suppl., Columbus, Ohio: American Ceramic Society, Fig. 1428 2 周国治,李瑞青.稀有金属,待发表 3 Barin I, Knacke O, Kubaschewski O. Thermochemical Properties of Inorganic Substances, Springer-Verlag, Berlin, 1977 4 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists, and 1969, 1975 Suppl., Columbus, Ohio: American Ceramic Society, Fig. 1311 5 Emons H H, Brautigan G, Thomas R. Chem Zvesti, 1978; 32 (6) : 721 6 1968; 13 (8) ; 2251 7 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists, and 1969, 1975 Suppl., Columbus. Ohio: American Ceramic Society, Fig. 1301 8 Egan J J. Bracker J. J Chem Thermodyn, 1974; 6: 9 9 Qiao Zhiyu (乔芝郁), James Sangster. Pelton A D. CALPHAD, 1987; 11: 10 Papatheodorou G N. Kleppa O J. J Chem Phys, 1967; 47: 2014 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|