Please wait a minute...
Acta Metall Sin  1989, Vol. 25 Issue (2): 152-154    DOI:
Current Issue | Archive | Adv Search |
THERMODYNAMIC PROPERTIES OF Fe-V-Ce LIQUID SOLUTION
CHANG Heming;DU Ting;YU Jingsheng Central Iron and Steel Research Institute; Beijing
Cite this article: 

CHANG Heming;DU Ting;YU Jingsheng Central Iron and Steel Research Institute; Beijing. THERMODYNAMIC PROPERTIES OF Fe-V-Ce LIQUID SOLUTION. Acta Metall Sin, 1989, 25(2): 152-154.

Download:  PDF(193KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Reaction of Ce with S and O in liquid Fe-V-Ce solution has beenstudied in the temperature range of 1550 to 1670℃. The temperature dependences ofthe equilibrium constant of reaction Ce_2O_2S=2(Ce)+2(O)+(S) and the starndard freeenergy of formation of Ce_2O_2S have been obtained. The temperature dependences ofthe interaction coefficients e_V~(Ce) and e_(Ce)~V. have also been determined.
Key words:  Fe-V-Ce system      thermodynamics      activity      interaction coefficient     
Received:  18 February 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I2/152

1 周谦莉,杜挺,金属学报,1989;25(1) ;
2 Savitskii E M. Baron VV. Efimov Yu V. Eng Transl Russ J Inorg Chem, 1962: 7; 359
3 乐可襄,杜挺,李继宗,沈汝美,金属学报,1987;23:A99
4 Wu Yieming, Wang Longmei, Du Ting. J Less-Common Met, 1985; 110: 187
5 韩其勇,北京钢铁学院学报,1986;(3) :115
6 Sigworth G K, Elliott J F. Met Sci, 1974; 8: 298
7 Elliott J F. Electr Furnace Conf Proc, 1974; 32: 62
8 Gibson J. Properties of the Rare Earth Metals and Compounds, 1966: 59~
[1] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[2] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[3] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[4] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[5] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[6] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[7] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[8] Muqin LI, Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG. The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. 金属学报, 2017, 53(10): 1337-1346.
[9] Xiaofeng LU, Ming XIAO, Yangmei CHEN, Bangcheng YANG. Bioactivity of Titanium Metal Hybridized with Inactivated Bacterial Biofilm[J]. 金属学报, 2017, 53(10): 1402-1412.
[10] Liheng LIU,Chunshan CHE,Gang KONG,Jintang LU,Shuanghong ZHANG. DESTABILIZATION MECHANISM OF Fe-Al INHIBITION LAYER IN Zn-0.2%Al HOT-DIP GALVANIZING COATING AND RELATED THERMODYNAMIC EVALUATION[J]. 金属学报, 2016, 52(5): 614-624.
[11] Feng LIU, Kang WANG. DISCUSSIONS ON THE CORRELATION BETWEEN THERMODYNAMICS AND KINETICS DURING THE PHASE TRANSFORMATIONS IN THE TMCP OF LOW-ALLOY STEELS[J]. 金属学报, 2016, 52(10): 1326-1332.
[12] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[13] XIE Jun, YU Jinjiang, SUN Xiaofeng, JIN Tao, SUN Yuan. CARBIDE EVOLUTION BEHAVIOR OF K416B AS-CAST Ni-BASED SUPERALLOY WITH HIGH W CONTENT DURING HIGH TEMPERATURE CREEP[J]. 金属学报, 2015, 51(4): 458-464.
[14] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[15] WU Changjun, ZHU Chenlu, SU Xuping, LIU Ya, PENG Haoping, WANG Jianhua. THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION[J]. 金属学报, 2014, 50(8): 930-936.
No Suggested Reading articles found!