DISTRIBUTION OF SULFUR IN HIGH TEMPERATURE PHASES OF CAST IRON
HAN Qiyong;YANG Ping;SONG Weixi Beijing University of Science and Technology
Cite this article: 

HAN Qiyong;YANG Ping;SONG Weixi Beijing University of Science and Technology. DISTRIBUTION OF SULFUR IN HIGH TEMPERATURE PHASES OF CAST IRON. Acta Metall Sin, 1989, 25(1): 86-90.

Download:  PDF(1892KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In grey cast iron, sulfur is concentrated in the liquid, flake graphiteand on the edge of D-type supercooled graphite eutectic cells, but less sulfur is inaustenite. Besides, the content of sulfur in A-type graphite is higher than that inDtyp graphite, and the sulfur content in eutectic austenite is a little higher thanthat in primary austenite. While in nodular cast iron, less sulfur is in liquid andaustenite, but more in nodular graphite.
Key words:  cast iron      autoradiograph      sulfur      graphite     
Received:  18 January 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I1/86

1 方克明,倪瑞明,李宝山,冯小亮.球铁,1984;(1) :16
2 秦子强.北京钢铁学院硕士论文,1986
3 张钟植.吉林工业大学硕士论文,1986
4 霍成章,韩其勇,钟伟珍,李宝山.中国稀土学报,1986;4(1) :53
5 韩其勇,吴卫江,方克明,卢静,张保军,谢德义,裴丽侠.金属学报,1979;15:1
[1] ZHANG Shihong, HU Kai, LIU Xia, YANG Yang. Corrosion-Erosion Mechanism and Research Prospect of Bare Materials and Protective Coatings for Power Generation Boiler[J]. 金属学报, 2022, 58(3): 272-294.
[2] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[3] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[4] Hongchi MA, Cuiwei DU, Zhiyong LIU, Yong LI, Xiaogang LI. Comparative Study of Stress Corrosion Cracking Behaviors of Typical Microstructures of Weld Heat-Affected Zones of E690 High-Strength Low-Alloy Steel in SO2-Containing Marine Environment[J]. 金属学报, 2019, 55(4): 469-479.
[5] Xiaoyun LIU,Wenguang WANG,Dong WANG,Bolv XIAO,Dingrui NI,Liqing CHEN,Zongyi MA. Effect of Graphite Flake Size on the Strength and Thermal Conductivity of Graphite Flakes/Al Composites[J]. 金属学报, 2017, 53(7): 869-878.
[6] Dahai XIA, Shizhe SONG, Jianqiu WANG, Jingli LUO. Research Progress on Sulfur-Induced Corrosion of Alloys 690 and 800 in High Temperature and High Pressure Water[J]. 金属学报, 2017, 53(12): 1541-1554.
[7] Wei FU,Xiaoguo SONG,Long LONG,Jianhang CHAI,Jicai FENG,Guodong WANG. INTERFACIAL MICROSTRUCTURE AND MECHANI-CAL PROPERTIES OF INDIRECT BRAZED GRAPHITE/COPPER JOINT[J]. 金属学报, 2016, 52(6): 734-740.
[8] ZHANG Lei, ZHAO Honglei, ZHU Mingfang. SIMULATION OF SOLIDIFICATION MICROSTRUC-TURE OF SPHEROIDAL GRAPHITE CAST IRON USING A CELLULAR AUTOMATON METHOD[J]. 金属学报, 2015, 51(2): 148-158.
[9] XUE Yingyu, TANG Jiancheng, ZHUO Haiou, YE Nan, WU Tong, ZHOU Xusheng. MICROSTRUCTURES AND PROPERTIES OF LEAD-FREE FREE-CUTTING GRAPHITE-BRASS PREPARED BY GRAPHITIZATION OF CEMENTITE[J]. 金属学报, 2015, 51(2): 223-229.
[10] Xinning ZHANG,Yingdong QU,Rongde LI,Junhua YOU. MECHANISM OF CRACK NUCLEATION AND PROPA- GATION OF FERRITE DUCTILE IRON DURING IMPACT FRACTURE UNDER LOW TEMPERATURES[J]. 金属学报, 2015, 51(11): 1333-1340.
[11] XU Kuangdi XIAO Lijun GAN Yong LIU Liu WANG Xinhua. THEORY ANALYSIS ON THE NEW GENERATION OF CLEAN STEEL PRODUCTION PROCESS[J]. 金属学报, 2012, 48(1): 1-10.
[12] SHAO Xiaojing WANG Xinhua JIANG Min WANG Wanjun HUANG Fuxiang JI Yunqing. IN SITU OBSERVATION OF MnS INCLUSION BEHAVIOR IN RESULFURIZED FREE-CUTTING STEEL DURING HEATING[J]. 金属学报, 2011, 47(9): 1210-1215.
[13] WANG Li-Min SUN Ming-Yuan. Electronical measurement of incision iron specimens’ fracture proceeding and calculation of the structure bearing capacity[J]. 金属学报, 2008, 44(7): 853-858 .
[14] YANG Jie; DONG Huaiyu; XIONG Shoumei. PREDICTION OF SHRINKAGE CAVITY AND POROSITY IN GRAY CAST IRON DURING SOLIDIFICATION[J]. 金属学报, 2005, 41(9): 929-932 .
[15] CHU Shaojun; LIU Haihong; ZHANG Heyi (Metallurgical Engineering College;University of Science and Technology Beijing; Beijing 100083)Correspondent: CHU Shaojun; associate professor; Tel: (010)62332790; Fax: (010)62522845. GRAPHITE NODULAR PHENOMENA DURING THE ESR OF CAST IRON[J]. 金属学报, 1998, 34(9): 971-976.
No Suggested Reading articles found!