PRE-TRANSITION AND PSEUDO-ELASTICITY IN NiTi (Fe) ALLOY
SHEN Huimin;HU Meishen;GUI Jianmin;YUAN Fang;WANG Yening;GUO Jinfang;QIAN Dongfan Institute of Solid State Physics; Nanjing University; General Research Institute for Non-Ferrous Metals; Beijing
Cite this article: 

SHEN Huimin;HU Meishen;GUI Jianmin;YUAN Fang;WANG Yening;GUO Jinfang;QIAN Dongfan Institute of Solid State Physics; Nanjing University; General Research Institute for Non-Ferrous Metals; Beijing. PRE-TRANSITION AND PSEUDO-ELASTICITY IN NiTi (Fe) ALLOY. Acta Metall Sin, 1988, 24(2): 84-88.

Download:  PDF(636KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The pseudo-elasticity of NiTi(Fe) alloy has been studied at diffe-rent temperatures and the stressed in situ X-ray and electron diffraction analysishave been performed at room temperature. The following results were obtained: (1)Above incommensurate transition temperature T_i, the stress-strain curve appears assuperelastic loop of small loop area, due to the stress induced incommensurate phaseas confirmed by in situ electron microscope experiment. (2) When R_s≤T
Key words:  NiTi alloy      phase transition      pseudo-elasticity     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/84

1 Salamon M B, Meichle M, Wayman C M, Hwang C M, Shapiro M. In: Cowley J M, Cohen J B, Salamon M B, Wuensch B J eds. Modulated Structures-1979, AIP Conf Proc, №53, New York: American Institute of Physics, 1979: 223
2 Moine P, Allain J. Renker B. J Phys F: Met Phys. 1984; 14: 2517
3 Mercier O. Brueesch P, Bruehrer W. Helv Phys Acta, 1980; 53: 243
4 Tietze H, Muellner M, Renker B. J Phys C: Solid State Phys, 1984; 17(21--24) : L529
5 Wang Yening (王业宁), Gui Jianmin (桂建敏). ICOMAT-86 Japan Institute of Metals, 1987 (待发表)
6 Gui Jianmin (桂建敏), Wang Yening (王来宁). J Phys (Parls). 1985; 46: C10--641
7 Ling H C, Kaplow R. Metall Trans, 1981; 12A: 2101
[1] HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si. Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. 金属学报, 2021, 57(4): 542-552.
[2] ZHANG Shaohua, XIE Guang, DONG Jiasheng, LOU Langhong. Investigation on Eutectic Dissolution Behavior of Single Crystal Superalloy by Differential Scanning Calorimetry[J]. 金属学报, 2021, 57(12): 1559-1566.
[3] WANG Chao, ZHANG Xu, WANG Yumin, YANG Qing, YANG Lina, ZHANG Guoxing, WU Ying, KONG Xu, YANG Rui. Mechanisms of Interfacial Reaction and Matrix Phase Transition in SiCf /Ti65 Composites[J]. 金属学报, 2020, 56(9): 1275-1285.
[4] Feng LIU, Linke HUANG, Yuzeng CHEN. Concurrence of Phase Transition and Grain Growth in Nanocrystalline Metallic Materials[J]. 金属学报, 2018, 54(11): 1525-1536.
[5] Zhaozhao WEI, Xiao MA, Xinping ZHANG. Topological Modelling of the B2-B19' Martensite Transformation Crystallography in NiTi Alloy[J]. 金属学报, 2018, 54(10): 1461-1470.
[6] WANG Shaobo, LIU Danmin, XIAO Weiqiang, ZHANG Zhenlu, YUE Ming, ZHANG Jiuxing. RESEARCH OF THE MAGNETOCALORIC PROPER- TIES IN Mn1.2Fe0.8P0.74Ge0.26-xSex COMPOUNDS[J]. 金属学报, 2014, 50(9): 1109-1114.
[7] ZHANG Meng, LIU Danmin, LIU Cuixiu, HUANG Qingzhen, WANG Shaobo, ZHANG Hu, YUE Ming. RESEARCH OF THE RELATIONSHIP BETWEEN PHASE TRANSITION PROCESS AND MAGNETIC PROPERTIES IN MAGNETIC REFRIGERATION MATERIAL Mn1.2Fe0.8P0.76Ge0.24[J]. 金属学报, 2013, 49(7): 783-788.
[8] PENG Yun WANG Aihua XIAO Hongjun TIAN Zhiling. EFFECT OF Cu ON MICROSTRUCTURE FORMING AND REFINING OF WELD METAL IN 690 MPa GRADE HSLA STEEL[J]. 金属学报, 2012, 48(11): 1281-1289.
[9] WANG Dongmei SONG Lin WANG Yaohui ZHANG Wei Bilige Tegus O. MAGNETOCALORIC EFFECT IN MnFeP0.63Ge0.12Si0.25Bx (x=0, 0.01, 0.02, 0.03) COMPOUNDS[J]. 金属学报, 2011, 47(3): 344-348.
[10] LIU Yihu WU Yongquan SHEN Tong WANG Zhaoke JIANG Guochang. MOLECULAR DYNAMICS SIMULATION OF PHASE TRANSFORMATION of  γ-Fe→δ-Fe→LIQUID–Fe IN CONTINUOUS TEMPERATURE–RISE PROCESS[J]. 金属学报, 2010, 46(2): 172-178.
[11] LI Da-Sheng; yupeng zhang; zhipeng xiong; Xinping Zhang. LOW DENSITY AND HIGH STRENGTH NiTi MEMORY ALLOYS WITH CONTROLLABLE PORE CHARATERISTICS AND THEIR SUPERELASTICITY[J]. 金属学报, 2008, 44(8): 995-1000 .
[12] Qian-Hua Kan; Guozheng Kang. EXPERMENTAL STUDY ON TRANSFORMATION RATCHETING OF SUPERELASTIC NITI ALLOY[J]. 金属学报, 2008, 44(8): 949-955 .
[13] CHENG Xuan. Phase Transitions of PLZT Ceramics near MPB Observed by In-situ Raman Spectroscopy[J]. 金属学报, 2008, 44(1): 29-33 .
[14] ;. HOT DEFORMATION BEHAVIOR AND CONSTITUTIVE RELATIONSHIP OF NiTi SHAPE MEMORY ALLOY DURING COMPRESSION AT ELEVATED TEMPERATURES[J]. 金属学报, 2007, 43(9): 930-936 .
[15] . Correcting of Hot Compression Test and Constitutive Equation of NiTi SMA[J]. 金属学报, 2006, 42(10): 1036-1040 .
No Suggested Reading articles found!