| DEFORMATION BANDS ON SURFACE OF NIOBIUM SINGLE CRYSTALS DURING CYCLIC DEFORMATION |
| LIN Dongliang (T. L. Lin)Professar;Dept.of Materials Science.Shanghai Jiaotong University;WU Jiansheng Shanghai Jiaotong University |
|
Cite this article:
LIN Dongliang (T. L. Lin)Professar;Dept.of Materials Science.Shanghai Jiaotong University;WU Jiansheng Shanghai Jiaotong University. DEFORMATION BANDS ON SURFACE OF NIOBIUM SINGLE CRYSTALS DURING CYCLIC DEFORMATION. Acta Metall Sin, 1988, 24(2): 76-83.
|
|
|
Abstract The surface morphology of niobium single crystals with [321]and [110] orientations during the deformation has been observed. Specimens withround cross section have been cycled to the saturated stage and the surface topog-raphy of rumpled bands has been observed using optical and scanning electron mi-croscope. In the present paper, the term of "deformation band", which is defferentfrom the kink band with special orientation, is used to define the rumpled band ofmaterial that has undergone inhomogenous plastic deformation. According to thedetailed topography, the deformation bands have been further subdivided into fivetypes and their formation process has been discussed. The deformation bands lie onthe plane of approximately 45° to the loading axis, i. e. the plane of the maxi-mum shear stress, which indicates that the macroscopic state of stress plays an im-portant role on the formation of deformation bands.
|
|
Received: 18 February 1988
|
1 Saletore M, Taggart R. Mater Sce Eng, 1978; 36: 259 2 Mughrabi H, Herz K, Stark X. Int J Fract, 1981; 17: 193 3 Lin Dongliang, Wu Jiansheng, Chen Xianfeng. Mater Sci Eng, 1987; 85: 19 4 吴建生.博士学位论文.上海交通大学,1985 5 Orowan E. Nature (London), 1942; 149: 643 6 A.塞格,张宏图译.晶体的范性及其理论.北京:科学出版社,1963:121 7 Crocker A G, Abell J S. Phil Mag, 1976; 33: 305 8 Guiu P, Pratt P L. Phys Status Solidi, 1966; 15: 539 9 Keh A S. Phil Mag, 1965; 12: 9 10 Duesbery M S, Foxall P A. Phil Mag, 1969; 20: 719 11 Flewitt P E J, Crocker A G. Phil Mag, 1976; 34: 877 12 Anglada M, Guiu F. Phil Mag A, 1981; 44: 433 13 Doner M, Diprimio J C, Salkovitz E I. Acta Metall, 1973; 21: 1547 14 Cotrell A H,葛庭燧译.晶体中的范性流变.北京:科学出版社,1960:174 15 冯端,王业宁,丘第荣.金属物理,下册.北京:科学出版社,1975:647 16 Hirsch P B. Prog Met Phys, 1956; 6: 236 17 Tapetado E G, Loretto M H. Phil Mag, 1974; 30: 30 18 Kuhlmann-Wilsdorf D. Phys Status Solidi (a), 1978: 47: 639 |