EFFECT OF β-QUENCHING ON THE CORROSION RESISTANCE OF Zr-4 ALLOY IN LiOH AQUEOUS SOLUTION
SHEN Yuefeng1), YAO Meiy1, 2)i,  ZHANG Xin1), LI Qiang1, 2),  ZHOU Bangxin1, 2), ZHAO Wenjin3)
1) Institute of Materials, Shanghai University, Shanghai 200072
2) Laboratory for Microstructures, Shanghai University, Shanghai 200444
3) The Key Laboratory for Nuclear Fuel and Materials, Nuclear Power Institute of China, Chengdu 610041
Cite this article: 

SHEN Yuefeng YAO Meiyi ZHANG Xin LI Qiang ZHOU Bangxin ZHAO Wenjin. EFFECT OF β-QUENCHING ON THE CORROSION RESISTANCE OF Zr-4 ALLOY IN LiOH AQUEOUS SOLUTION. Acta Metall Sin, 2011, 47(7): 899-904.

Download:  PDF(1220KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  To investigate the effect of $\beta$--quenching on the corrosion behavior, Zr--4 specimens were
$\beta$--quenched and subsequently annealed at 480---600 ℃ for 2---200 h. The corrosion tests were carried out in
0.01 mol/L LiOH aqueous solution at 360 ℃/18.6 MPa. The microstructure of Zr--4 specimens and fracture
surface morphology of oxide films on the corroded specimens were observed by TEM and HRSEM,
respectively. The results show that Zr--4 specimens exhibit excellent corrosion resistance as Zr--Sn--Nb
alloys in LiOH aqueous solution after increasing the solid solution content of Fe and Cr in $\alpha$--Zr matrix by
suitable quenching rate from $\beta$--phase to avoid the formation of $\beta$--Zr.
When the cooling rate is too fast, the specimens show worse corrosion resistance due to the formation
Key words:  &beta      -quenching     
Received:  13 April 2011     
ZTFLH: 

TL341

 
Fund: 

Supported by Defense Technology Key Laboratory Fund Project (No.9140C70040108C70), National\par Natural Science Foundation of China (No.50971084), High Technology Research and Development Program of China (No.2008AA031701), Natural Science Foundation of Shanghai (No.09ZR1411700) and Shanghai Leading Academic Discipline Project No.S30107)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2011.00233     OR     https://www.ams.org.cn/EN/Y2011/V47/I7/899

[1] Cox B, Wong Y M. In: Eucken C M, Garde A M, eds., Zirconium in the Nuclear Industry: 9th International Symposium, ASTM STP 1132, Baltimore: ASTM International, 1991: 643

[2] Pecheur D, Godlewski J, Peybernes J, Fayette L, Noe M, Frichet A, Kerrec O. In: Sabol G P, Moan G D, eds., Zirconium in the Nuclear Industry: 12th International Symposium, ASTM STP 1354, Philadelphia: ASTM International, 2000: 793

[3] Zhou B X, Li Q, Huang Q, Miao Z, Zhao W J, Li C. Nuc Power Eng, 2000; 21: 43

(周邦新, 李强, 黄强, 苗志, 赵文金, 李 聪. 核动力工程, 2000; 21: 43)

[4] Sabol G P, Comstock R J, Weiner R A, Larouere P, Stanutz R N. In: Garde A M, Bradley E R, eds., Zirconium in the Nuclear Industry: 10th International Symposium, ASTM STP 1245, Ann Arbor: ASTM International, 1994: 724

[5] Nikulina A V, Markelvo V A, Peregud M M, Bibilashvili Y K, Kotrekhov V A, Lositsky A F, Kuzmenko N V, Shevnin YP, ShamardinVK, KobylyanskyGP, NovoselovAE. In: Bradley E R, Sabol G P, eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International, 1996: 785

[6] Zhao W J, Miao Z, Jiang H M, Yu X W, Li W J, Li C, Zhou B X. J Chin Soc Corros Prot, 2002; 22: 124

(赵文金, 苗 志, 蒋宏曼, 于晓卫, 李卫军, 李聪, 周邦新. 中国腐蚀与防护学报, 2002; 22: 124)

[7] Li Z K, Liu J Z, Li P Z, Zhou L, Song Q Z. Rare Met Mater Eng, 1999; 28: 101

(李中奎, 刘建章, 李佩志, 周廉, 宋启忠. 稀有金属材料与工程, 1999; 28: 101)

[8] Li Z K, Liu J Z, Zhu M S, Song Q Z. Rare Met Mater Eng, 1996; 25: 43

(李中奎, 刘建章, 朱梅生, 宋启忠. 稀有金属材料与工程, 1996; 25: 43)

[9] Yao M Y, Zhou B X, Li Q, Liu W Q, Geng X, Lu Y P. J Nucl Mater, 2008; 374: 197

[10] Yao M Y, Zhou B X, Li Q, Liu W Q, Wang S A, Huang X S. Rare Met Mater Eng, 2007; 36: 1915

(姚美意, 周邦新, 李 强, 刘文庆, 王树安, 黄新树. 稀有金属材料与工程, 2007; 36: 1915)

[11] Zhou B X, Li Q, Miao Z. Nucl Power Eng, 2000; 21: 339

(周邦新, 李强, 苗 志. 核动力工程, 2000; 21: 339)

[12] Anada H, Herb B J, Nomoto K, Hagi S, Graham R A, Kuroda T. In: Bradley E R, Sabol G P, eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International, 1996: 74

[13] Foster P, Dougherty J, Burke M G, Bates J F, Worcester S. J Nucl Mater, 1990; 173: 164

[14] Garzarolli G, Steinberg E, Weidinger H G. In: Van Swam L F P, Eucken C M, eds., Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, Baltimore: ASTM International, 1989: 202

[15] Zhou B X, Zhao W J, Miao Z, Pan S F, Li C, Jiang Y R. Chin J Nucl Sci Eng, 1995; 15: 242

(周邦新, 赵文金, 苗志, 潘淑芳, 李 聪, 蒋有荣. 核科学与工程, 1995; 15: 242)

[16] Choo K N, Kang Y H, Pyun S I, Vrbanic V F. J NuclMat, 1994; 209: 226

[17] Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1

[18] Garzarolli F, Pohlmeyer I, Steinberg E, Trapp–pritsching S. Proc Technical Committee Meeting, Cadarache: the International Atomic Energy Agency, 1985: 66

[19] Liu J Z. Structure Nuclear Materials. Beijing: Chemical Industry Press, 2007: 111

(刘建章. 核结构材料. 北京: 化学工业出版社, 2007: 111)

[20] Yao M Y,Wang J H, Peng J C, Zhou B X, Li Q. J ASTM Intl, 2011; 8: 13

[21] Liu W Q, Li Q, Zhou B X, Yao M Y. Rare Met Mater Eng, 2004, 33: 728

(刘文庆, 李强, 周邦新, 姚美意. 稀有金属材料与工程, 2004, 33: 728)

[22] Zhou B X, Li Q, Yao M Y, Liu WQ, Chu Y L. Nucl Power Eng, 2005; 26: 364

(周邦新, 李强, 姚美意, 刘文庆, 褚于良. 核动力工程, 2005; 26: 364)

[23] Zhou B X, Li Q, Liu W Q, Yao M Y, Chu Y L. Rare Met Mater Eng, 2006; 35: 1009

(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009)

[24] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. J ASTM Intl, 2008; 5: 360
[1] ZHANG Min,JIA Fang,CHENG Kangkang,LI Jie,XU Shuai,TONG Xiongwei. Influence of Quenching and Tempering on Microstructure and Properties of Welded Joints of G520 Martensitic Steel[J]. 金属学报, 2019, 55(11): 1379-1387.
[2] LI Qun, WANG Qing, LI Xiaona, GAO Xiaoxia, DONG Chuang. INFLUENCES OF PHASE PRECIPITATIONS OF TERNARY βTi-Mo-Zr(Sn) ALLOYS ON YOUNG'S MODULUS AND MECHANICAL PROPERTIES[J]. 金属学报, 2013, 49(9): 1143-1147.
[3] ZHENG Junzi, ZHANG Laiqi, HOU Yongming, MA Xiangling, LIN Junpin. QUASI ISOTHERMAL FORGING SIMULATION OF β-γ TiAl ALLOY CONTAINING HIGH CONTENT OF Nb[J]. 金属学报, 2013, 49(11): 1439-1444.
[4] WANG Jinhong WANG Rongshan WENG Likui ZHANG Yanwei GENG Jianqiao. HYDROGEN ABSORPTION AND DESORPTION PERFORMANCES OF THE SECOND PHASES IN ZIRCONIUM ALLOY WITH Nb[J]. 金属学报, 2011, 47(9): 1200-1204.
[5] LI Qiang LIANG Xue PENG Jianchao LIU Renduo YU Kang ZHOU Bangxin. OXIDATION BEHAVIOR OF THE β-Nb PHASE PRECIPITATED IN Zr-2.5Nb ALLOY[J]. 金属学报, 2011, 47(7): 893-898.
[6] MA Rentao HAO Chuanpu WANG Qing REN Mingfa WANG Yingmin DONG Chuang. CLUSTER-PLUS-GLUE-ATOM MODEL AND COMPOSITION DESIGN OF BCC Ti-Mo-Nb-Zr SOLID SOLUTION ALLOYS WITH LOW YOUNG'S MODULUS[J]. 金属学报, 2010, 46(9): 1034-1040.
[7] YANG Wenchao WANG Mingpu SHENG Xiaofei ZHANG Qian WANG Zheng’an. STUDY OF THE AGING PRECIPITATION AND HARDENING BEHAVIOR OF 6005A ALLOY SHEET FOR RAIL TRAFFIC VEHICLE[J]. 金属学报, 2010, 46(12): 1481-1487.
[8] YANG Rui HAO Yulin Obbard E G DONG Limin LU Bin. ORTHORHOMBIC PHASE TRANSFORMATIONS IN TITANIUM ALLOYS AND THEIR APPLICATIONS[J]. 金属学报, 2010, 46(11): 1443-1449.
[9] KANG Mokuang ZHANG Mingxing LIU Feng ZHU Ming. OVERALL ACTIVATION ENERGY OF ISOTHERMAL TRANSFORMATION IN METAL ALLOY AND ITS MECHANISM II. Isothermal Transformation in β Brasses[J]. 金属学报, 2009, 45(1): 32-36.
[10] CHE Hiaozhou; HU Gengxiang(Shanghai Jiaotong University); CAO Hingguo(Luoyang Institute of Technology); DAI Lizhi(Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). ANNEALING EMBRITTLEMENT OF AMORPHOUS Fe-B-Si ALLOYS[J]. 金属学报, 1994, 30(24): 532-536.
[11] ZHOU Yigang; YU Hanqing; ZENG Weidong (Northwestern Polytechnical University; Xi'an)TANG Jialing (Chinese Aviation South Power Machine Company; Zhuzhou). EFFECT OF β-FLECK ON MECHANICAL PROPERTIES OF Ti-10V-2Fe-3Al ALLOY[J]. 金属学报, 1992, 28(12): 23-28.
No Suggested Reading articles found!