Al_2O_3-SiO_2系纤维增强ZL109合金复合材料的时效特性 |
张茂勋;陈晓;钱匡武;里达雄;神尾彰彦 |
福州大学;福州;350002;福州大学;福州;350002;福州大学;福州;350002;日本东京工业大学;日本东京工业大学 |
|
THE AGING CHARACTERS OF ZL 109 ALLOY MATRIX COMPOSITE RE1NFORCED WITH Al_2O_3-SiO_2, FIBRE |
ZHANG MaOxun; CHEN Xiao; QIAN Kuangwu (University Fuzhou; Fuzhou 350002); Tatsuo Sato; AKIHIKO Kamio (TOkyo Institute ofTechnology; Tokyo) (Manuscript received 1996-08-12; in revised form 1997-04-27) |
引用本文:
张茂勋;陈晓;钱匡武;里达雄;神尾彰彦. Al_2O_3-SiO_2系纤维增强ZL109合金复合材料的时效特性[J]. 金属学报, 1997, 33(8): 891-896.
,
,
,
,
.
THE AGING CHARACTERS OF ZL 109 ALLOY MATRIX COMPOSITE RE1NFORCED WITH Al_2O_3-SiO_2, FIBRE[J]. Acta Metall Sin, 1997, 33(8): 891-896.
1Dutta I, Haper C P. The 3rd International Con.krence on Aluminium Alloys, Trondheim, Norway,1992: 519 2 Edwards G A, Yao J Y, Couper M J, Dunlop G L. The 3rd International Conference on Aluminiumalloys, Trondheim, Norway, 1992: 525 3 Jingtao Wang, Minoru Furukawa, Zenji Horita, Minoru Nemoto, Yan Ma, Terence G L. MetallMater Trans, 1995; 26A: 581 4 CHEN Kuochan, CHAO Chuenguang. Metall Mater Trans,1995; 26A:1035 5 Dudek H J, Borath R, Kleine A. J Mater Sci, 1996; 31: 795 6神尾彰彦:组织性质.东京:轻金属学会出版社,1991:194 7 Augis J A, Bennett J E. J Thermal Anal, 1978; 13: 283L |
|