| 脉冲电流作用下TIG焊接熔池行为的数值模拟 |
| 武传松;郑炜;吴林 |
| 山东工业大学连接技术研究所;济南;250061;哈尔滨工业大学材料科学与工程学院;哈尔滨;150001;哈尔滨工业大学材料科学与工程学院;哈尔滨;150001 |
|
| NUMERICAL SIMULATION OF TIG WELD POOL BEHAVIOR UNDER THE ACTION OF PULSED CURRENT |
| WU Chuansong (Institute of Joining Technology; Shandong University of Technologyl Jinan 250061)ZHENG Wei; WU Lin(College of Materials Science and Engineering; Harbin Institute of Technology Harbin 150001) |
引用本文:
武传松;郑炜;吴林. 脉冲电流作用下TIG焊接熔池行为的数值模拟[J]. 金属学报, 1998, 34(4): 416-422.
,
,
.
NUMERICAL SIMULATION OF TIG WELD POOL BEHAVIOR UNDER THE ACTION OF PULSED CURRENT[J]. Acta Metall Sin, 1998, 34(4): 416-422.
1 Ramanan N,Korpela s A.Metall Trans,1990;21 A:45 2 Choo R T C, Szekely J Weld J, 1991; 70: 2235 3 Zacharia T. Metall Trans; 1991; 22B: 233 4武传松,曹振宁,吴林金属学报,1992;28:B428 (Wu Chuansong,Cao Zhenning,Wu Lin. Acta Metall Sin , 1992; 28:B428) 5 Wu C S,Dorn L.Comput Mater Sci ,1994;2:741 6 Domey J, Aidun D K. Weld J, 1995; 75: 263s 7郑 炜,武传松,吴林.材料科学与工艺,1996;4:15(Zheng Wei, Wu Chuansong, Wu Lin, Mater Sci Technol , 1996;4:15) 8殷树言,张九海.气体保护焊工艺.哈尔滨:哈尔滨工业大学出版社,1988:181 (Yin Shuyan, Zhang Jiuhai. Gas Shielded Arc Weldiny Technology. Harbin: Harbin Institute of Technology Press, 1988: 181) 9郑 炜.哈尔滨工业大学工学博士学位论文,1996 (Zheng Wei. Ph.D Thesis, Harbin Institute of Technology, 1996) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|