| 纳米复合磁体磁化过程的计算机研究 |
| 初业隆;熊良钺;孙校开 |
| 中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015 |
|
| COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS |
| CHU Yelong; XIONG Liangyue; SUN Xiaokai (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015) |
引用本文:
初业隆;熊良钺;孙校开. 纳米复合磁体磁化过程的计算机研究[J]. 金属学报, 1998, 34(4): 423-430.
,
,
.
COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS[J]. Acta Metall Sin, 1998, 34(4): 423-430.
1 McCallum R W, Kadin A M, Clemente G B, Keem J E. J Appl Phys, 1987; 61: 3577 2 Manaf A, Buckley R A, Davies H. J Magn Magn Mater, 1993; 128: 302 3 Kneller E P, Hawig R. IEEE bens Magn, 1992; MAG-27: 3588 4 Skomski R, Coey J M D. Phys Rev, 1993; 48B: 15812 5 Schrefl T, Fidler J, Kronmller H. Phys Rev, 1994; 49B: 6100 6 Liu W, Wang Q, Sun X K, Zhao X G, Zhao T, Zhang Z D, Chuang Y C. J Magn Magu Mater, 1994; 131: 413 7 Yang J L, Wang Q, Sun X K, Zeng G Y, Chen M, Liu W, Zhao X G, Zhso T, Zhang Z D. J Mop Magn Maten 1994; 134: 197 8 Jin Z Q, Sun X K, Liu W, Zhao X G, Xiao Q F, Sui Y C, Zhang Z D, Wang Z G, Qin H X. i Magn Magn Mater, 1997; 169: 135 9 Fukunaga H, Inoue H. Jpn J Appl Phgs, 1992; 31: 1347 10 Binder K, Heermann D W 著 秦克诚译. 统计物理学中的蒙特罗模拟方法. 北京:北京大学出版社, 1994: 33 (Binder K, Heermann D W ed, Qin Kecheng trans. Monte Carlo Simulation in Statistical Physics. Beijing:Peking Uni Press, 1994; 33) 11 Zijlstra H. In: Wohlfarth E P ed., Fermmagnetic Materiats, Vol.3., Amsterdam: N0rth-Holland Publishing, 1982: 37 12 Kronmller H. In: Long G J, Grandjcan F eds., Supermaguets, Hard Manetic Materiais, Dordrecht:Kluwer Academic Publisherrs, 1990: 461 13 Chudnovsky E M, In: Fernandez-baca J A, Ching Wai-Yim eds., The Manetism of Amorphous Metais and Alloys. Singapore: World Scientific, 1995: 143 14 Herzer G. IEEE Trans Magn, 1990; MAG-26: 1397 15 Otani Y, Li H S, Coey J M D. IEEE Trans Magn, 1990; MAG-26: 2658 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|