金属学报  2010, Vol. 46 Issue (1): 91-96    
  论文 本期目录 | 过刊浏览 |
连铸二冷区铸坯展宽现象的黏弹塑性分析
付建勋1;2);李京社1);张慧2)
1) 北京科技大学冶金与生态工程学院; 北京 100083
2) 中国钢研集团连铸技术国家工程研究中心; 北京 100081
VISCOELASTIC-PLASTIC ANALYSIS OF BROADENING OF SLAB IN THE SECONDARY COOLING ZONE OF CONTINUOUS CASTING
FU Jianxun1;2); LI Jingshe1); ZHANG Hui2)
1) School of Metallurgical and Ecological Engineering; University of Science and Technology Beijing; Beijing 100083
2) National Engineering Research Center of Continuous Casting Technology; China Iron $\&$ Steel Research Institute Group; Beijing 100081
引用本文:

付建勋 李京社 张慧. 连铸二冷区铸坯展宽现象的黏弹塑性分析[J]. 金属学报, 2010, 46(1): 91-96.
, , . VISCOELASTIC-PLASTIC ANALYSIS OF BROADENING OF SLAB IN THE SECONDARY COOLING ZONE OF CONTINUOUS CASTING[J]. Acta Metall Sin, 2010, 46(1): 91-96.

全文: PDF(992 KB)  
摘要: 

通过在商业软件MSC.Marc基础上二次开发, 建立了黏弹塑性三维热-力耦合有限元模型, 模拟铸坯在二冷区的展宽状况. 结果显示: 铸坯的展宽主要产生于二冷区的前段, 在前 6个扇形段, 铸坯的目标展宽率有逐渐增加的趋势; 铸坯的展宽与厚度方向上的鼓肚密切相关; 数值模拟使用的黏弹塑模型揭示铸坯展宽规律与铸坯实际变形相符, 铸坯展宽是坯壳在钢液芯静压力作用下发生黏弹塑变形的结果.

关键词 : 连铸,  板坯,  二冷区,  展宽,  热力耦合,  黏弹塑性    
Abstract:

The 3D viscoelastic-plastic thermal-mechanically coupled finite element model was established by a commercial software MSC.Marc on the basis of secondary development, and used to simulate the situation of slab's broadening in the secondary cooling zone. The results showed that the slab's broadening mainly emerged in the former segments of the secondary cooling zone, and the broadening rate has a gradually increasing trend from the first segment to the sixth segment. The broadening of slab has a close relationship with bulging along the thickness direction. The results simulated by using viscoelastic-plastic model revealed that the law of the slab's broadening is excellent agreement with the actual deformation. The broadening of slab is the result of viscoelastic-plastic deformation of the slab shell under the pressure of core of molten steel.

Key words: continuous casting    slab    secondary cooling zone    broadening    thermal-mechanical couple    viscoelastic-plasticity
收稿日期: 2009-07-20     
ZTFLH: 

TF777.7

 
基金资助:

国家“十一五”科技支撑计划资助项目2006BAE03A04

作者简介: 付建勋, 男, 1969年生, 副教授, 博士生

[1] Yoshii A, Kihara S. Trans ISIJ, 1986; 26: 891
[2] Maeno S, Wada K, Itoh Y, Nagano Y. Trans ISIJ, 1983; 24: 83
[3] Siyasiya C, van Rooyen G T. Stumpf W E. J South Afr Inst Mining Metall, 2005; 105: 473
[4] Lin Q Y, Zhu M Y. Acta Metall Sin, 2007; 43: 1301
(林启勇, 朱苗勇. 金属学报, 2007; 43: 1301)
[5] Chen Z P, Cheng N L, Cui L X, Zhang J Q. Iron Steel, 2004; 39(suppl): 457
(陈志平, 程乃良, 崔立新, 张家泉. 钢铁, 2004; 39(增刊): 457
[6] Fu J X. PhD Thesis, University of Science and Technology Beijing, 2009

(付建勋. 北京科技大学博士学位论文, 2009)
[7] Kim K H, Yeo T J, Oh K H, Lee D N. ISIJ Int, 1996; 36: 284
[8] Grill A, Schwerdtfeger K. Ironmak Steelmak, 1979; 6: 131
[9] Barber B, Lewis B A, Leckenby B M. Ironmak Steelmak, 1985; 12: 171
[10] Okamura K, Kawashima H. ISIJ Int, 1989; 29: 666
[11] Sorimachi K, Brimacombe J K. Ironmak Steelmak, 1977; 4: 240
[12] Wang X C. Finite Element Method. Beijing: Tsinghua University Press, 2003: 125
(王勖成. 有限单元法. 北京: 清华大学出版社, 2003: 125)

[13] Fu J X, Li J S, Wang C L, Zhu J T. Mater Rev, 2009; 23(9): 68
(付建勋, 李京社, 汪春雷, 朱经涛. 材料导报, 2009; 29(9): 68)
[14] Uehara M, Samarasekera I V, Brimacombe J K. Iro nmak Steelmak, 1986; 13: 138
[15] Chen S Q. PhD Thesis, Central Iron and Steel Research Institute, Beijing, 2004

(陈素琼. 钢铁研究总院博士学位论文, 北京, 2004)

[1] 彭治强, 柳前, 郭东伟, 曾子航, 曹江海, 侯自兵. 基于大数据挖掘的连铸结晶器传热独立变化规律[J]. 金属学报, 2023, 59(10): 1389-1400.
[2] 郭东伟, 郭坤辉, 张福利, 张飞, 曹江海, 侯自兵. 基于二次枝晶间距变化特征的连铸方坯CET位置判断新方法[J]. 金属学报, 2022, 58(6): 827-836.
[3] 李民, 李昊泽, 王继杰, 马颖澈, 刘奎. 稀土Ce对薄带连铸无取向6.5%Si钢组织、高温拉伸性能和断裂模式的影响[J]. 金属学报, 2022, 58(5): 637-648.
[4] 刘中秋, 李宝宽, 肖丽俊, 干勇. 连铸结晶器内高温熔体多相流模型化研究进展[J]. 金属学报, 2022, 58(10): 1236-1252.
[5] 郭中傲, 彭治强, 柳前, 侯自兵. 高碳钢连铸坯大区域C元素分布不均匀度[J]. 金属学报, 2021, 57(12): 1595-1606.
[6] 唐海燕, 刘锦文, 王凯民, 肖红, 李爱武, 张家泉. 连铸中间包加热技术及其冶金功能研究进展[J]. 金属学报, 2021, 57(10): 1229-1245.
[7] 蔡来强, 王旭东, 姚曼, 刘宇. 连铸圆坯非均匀传热/凝固行为的无网格计算方法[J]. 金属学报, 2020, 56(8): 1165-1174.
[8] 任忠鸣,雷作胜,李传军,玄伟东,钟云波,李喜. 电磁冶金技术研究新进展[J]. 金属学报, 2020, 56(4): 583-600.
[9] 李亚强, 刘建华, 邓振强, 仇圣桃, 张佩, 郑桂芸. 15CrMoG钢包晶凝固特征与机制[J]. 金属学报, 2020, 56(10): 1335-1342.
[10] 吴春雷,李德伟,朱晓伟,王强. 电磁旋流水口连铸技术对小方坯凝固组织形貌和宏观偏析的影响[J]. 金属学报, 2019, 55(7): 875-884.
[11] 郭军力, 文光华, 符姣姣, 唐萍, 侯自兵, 谷少鹏. 冷却速率对包晶钢凝固过程中包晶转变收缩的影响[J]. 金属学报, 2019, 55(10): 1311-1318.
[12] 侯自兵, 徐瑞, 常毅, 曹江海, 文光华, 唐萍. 高碳钢连铸方坯拉坯方向偏析C元素分布的时间序列波动特征[J]. 金属学报, 2018, 54(6): 851-858.
[13] 刘新华, 付华栋, 何兴群, 付新彤, 江燕青, 谢建新. Cu-Al复合材料连铸直接成形数值模拟研究[J]. 金属学报, 2018, 54(3): 470-484.
[14] 朱苗勇, 娄文涛, 王卫领. 炼钢与连铸过程数值模拟研究进展[J]. 金属学报, 2018, 54(2): 131-150.
[15] 王强, 何明, 朱晓伟, 李显亮, 吴春雷, 董书琳, 刘铁. 电磁场技术在冶金领域应用的数值模拟研究进展[J]. 金属学报, 2018, 54(2): 228-246.