| 环氧树脂修饰微米片状Fe粉的制备与电磁性能 |
| 董德明; 官建国; 王维; 李维; 周静 |
| 武汉理工大学材料复合新技术国家重点实验室; 武汉 430070 |
|
| PREPARATION AND ELECTROMAGNETIC PROPERTIES OF MICROMETER Fe FLAKES MODIFIED WITH EPOXY RESIN |
| DONG Deming; GUAN Jianguo; WANG Wei; LI Wei; ZHOU Jing |
| State Key Laboratory of Advanced Technology for Materials Synthesis and Processing; Wuhan University of Technology;Wuhan 430070
|
引用本文:
董德明 官建国 王维 李维 周静. 环氧树脂修饰微米片状Fe粉的制备与电磁性能[J]. 金属学报, 2009, 45(9): 1141-1145.
,
,
,
,
.
PREPARATION AND ELECTROMAGNETIC PROPERTIES OF MICROMETER Fe FLAKES MODIFIED WITH EPOXY RESIN[J]. Acta Metall Sin, 2009, 45(9): 1141-1145.
| [1] Yoshida S, Sato M, Sugawara E, Shimada Y. J Appl Phys, 1999; 35: 4636
[2] Hashimoto O, Takase Y, Haga S. Trans IEICE Jpn, 2003; 86B: 113
[3] Smit J, Wijn H P J. Ferrites. Eindhoven: Philips Technical Library, 1959: 78
[4] Naito Y, Suetake K. IEEE Trans Microwave Theory Technol, 1971; 19: 65
[5] Zhang X N. PhD Thesis, Beijing University of Technology, 2003
(张晓宁. 北京工业大学博士学位论文, 2003)
[6] Nie Y, He H H, Zhao Z S, Gong R Z, Yu H B. J Magn Magn Mater, 2006; 306: 125
[7] Xie J L, Lu C L, Deng L J. Acta Mater Compos Sin, 2007; 24: 18
(谢建良, 陆传林, 邓龙江. 复合材料学报, 2007; 24: 18)
[8] Wang Q, Guan J G, Liu Q, Wang W, Zhang Q J. J Alloy Compd, 2006; 413: 155
[9] Tong G X,Wang W, Guan J G, Zhang Q J. J InorgMater, 2006; 21: 1461
(童国秀, 王 维, 官建国, 张清杰. 无机材料学报, 2006; 21: 1461)
[10] Jiang M J, Dang Z M, Yao S H, Bai J B. Chem Phys Lett, 2008; 457: 352
[11] Zhang Q Y, Zhang H P, Xie G, Zhang J P. J Magn Magn Mater, 2007; 311: 140
[12] Jiang M J, Dang Z M, Xu H P. Eur Polym J, 2007; 43: 4924
[13] Li H Y, Wang R G, Hu H L, Liu W B. Appl Surf Sci, 2008; 255: 1984
[14] Mittal V, Herle V. J Colloid Interface Sci, 2008; 327: 295
[15] Dash S, Mishra S, Patel S, Mishra B K. Adv Colloid Interface, 2008; 140: 77
[16] Vrkoslav V, Jel´?nek I, Trojan T, Jindˇrich J, Dian J. Physica, 2007; 38E: 200
[17] Walser R M, KangW. IEEE Trans Magn, 1998; 34: 1144
[18] Musal H M, Hahn H T. IEEE Trans Magn, 1989; 25: 3851 |
|