| Fe-Al合金中与Al反位置原子弛豫有关的内耗峰 |
| 孙蔚 韩福生 吴杰 |
| 浙江工贸职业技术学院; 温州325003 |
|
| The internal friction peak correlated to the relaxation of Al antisite atoms in Fe-Al alloys |
| SUN Wei |
| Zhejiang Industry and Trade Polytechnic College; Wenzhou 325003 |
引用本文:
孙蔚; 韩福生; 吴杰 . Fe-Al合金中与Al反位置原子弛豫有关的内耗峰[J]. 金属学报, 2007, 43(3): 311-314 .
,
,
.
The internal friction peak correlated to the relaxation of Al antisite atoms in Fe-Al alloys[J]. Acta Metall Sin, 2007, 43(3): 311-314 .
[1]de Diego N,Plazaola F,Jimnez J A,Serna J,R(?)o J D. Acta Mater,2005;53:163 [2]Deevi S C,Sika V K.Intermetallics,1996;4:357 [3]Wolff J,Franz M,Broska A,Kerl R,Weinhagen M,K(?)hler B,Brauer M,Faupel F,Hehenkamp Th.Intermetallics, ??1999;7:289 [4]Chang Y A,Pike L M,Liu C T,Bilbrey A R,Stone D S. Intermetallics,1993;1:107 [5]Schaefer H-E,Frenner K,W (?) rshum R.Phys Rev Lett, 1999;82:948 [6]W(?)rshum R,Grupp C,Schaefer H E.Phys Rev Lett,1995; 75:97 [7]Schaefer H E,Damson B,Weller M,Arzt E,George E P. Phys Status Solidi,1997;160a:531 [8]Blanter M S,Golovin I S,Sinning H R.Scr Mater,2005; 52:57 [9]Golovin I S,Divinski S V,(?)ek J,Procházka I,Stein F. Acta Mater,2005;53:2581 [10]Han F S,Zhu Z G,Gao J C.Metall Mater Trans,1999; 30 A:771 [11]Nowick A S,Berry B S.Anelastic Relaxation in Crys- talline Solids.New York:Academic Press,1972 [12]Bevington P R.Data Reduction and Error Analysis for the Physical Science.New York:McGraw-Hill,1969:235 [13]Kubaschewski O.Iron-Binary Phase Diagrams.Berlin: Springer,1982 [14]Fu C L.Phys Rev,1995;52B:3151 [15]Fu C L,Ye Y Y,Yoo M H,Ho K M.Phys Rev,1993;48 B:6712 [16] Wu J,Han F S,Gao Z Y,Hao G L,Wang Q Z.Phys Status Solidi,2006;203a:485 [17]Haraguchi T,Yoshimi K,Yoo M H,Kato H,Hanada S, Inoue A.Acta Mater,2005;53:3751 [18]Zhou Z C,Han F S,Gao Z Y.Acta Mater,2004;52:4049 [19]Kogachi M,Haraguchi T.Mater Sci Eng,1997;A230:124 [20]Lang H,Rohrhofer K,Rosenkranz P,Kozubski R,P(?)schl W,Pfeiler W.Intermetallics.2002;10:283 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|