| 预压缩对镍基单晶高温合金DD98持久性能的影响及其作用机理 |
| 刘金来;金 涛;孙晓峰;张静华;管恒荣;胡壮麒 |
| 中科院金属研究所 |
|
| Effect of pre-compression on the stress rupture properties of single crystal superalloy:Ⅰmicrostructure and stress rupture properties of pre-compressed samples |
| 中科院金属研究所 |
引用本文:
刘金来; 金涛; 孙晓峰; 张静华; 管恒荣; 胡壮麒 . 预压缩对镍基单晶高温合金DD98持久性能的影响及其作用机理[J]. 金属学报, 2006, 42(8): 843-849 .
[1]Pollock T M,Argon A S.Acta Metall Mater,1992;40:1 [2]Srinivasan R,Eggeler G F,Mills M J.Acta Mater,2000;48:4867 [3]Fredholm A,Strudel J L.In:Gell M,Kortvich C S,Bricknell R H,Kent W B,Radavich J F,eds.,Superalloys 1984,Warrendale,PA:AIME,1984:211 [4]Pollock T M,Argon A S.Acta Metall Mater,1994;42:1859 [5]Peng Z F,Feller-Kniepmeier M.Acta Metall Sin,1995;31:371 (彭志方,Feller-Kniepmeier M.金属学报,1995;31:371) [6]Matan N,Cox D C,Rae C M F,Reed R C.Acta Mater,1999;47:2031 [7]Mughrabi H,Ott M,Tetzlaff U.Mater Sci Eng,1997;A234:434 [8]Tetzlaff U,Mughrabi H.In:Pollock T M,Kissinger R D,Bowman R R,Green K A,McLean M,Olson S L,Schirra J J,eds.,Superalloys 2000,Warrendale,PA:TMS,2000:273 [9]Nathal M,MacKay R,Miner R.Trans Metall,1989;20A:133 [10]Pearson D,Lemkey F,Kear B.In:Tien J K,Wlodek S T,MorrowⅢH,eds.,Superalloys 1980,Warrendale,PA:AIME,1980:513 [11]Schneider W,Hammer J,Mughrabi H.In:Antolovich S D,Stusrud R W,Mackay R A,Anton D L,Khan T,Kissinger R D,Klarstrom D L,eds.,Superalloys 1992,Warrendale,PA:TMS,1992:589 [12]Mughrabi H,Schneider W,Sass V,Lang C.In:Oikawa H,Maruyama K,Takeuchi S,Yamaguchi M,eds.,Proc 10th Int Conf Strength of Metals and Alloys,ICSMA 10,Sendai,Japan:Japan Institute of Metals,1994:705 [13]Veron M,Brechet Y,Louchet F.In:Kissinger R D,Nathal M V,Deye D J,Pollock T M,Anton D L,woodford D A,Cetel A D,eds.,Superalloys 1996,Warrendale,PA:TMS,1996:181 [14]Zhang J X,Wang J C,Harada H,Koizumi Y.Acta Mater,2005;53:4623 [15]Sherry A H,Pilkington R.Mater Sci Eng,1993;A172:51 [16]Liu J L,Jin T,Zhang J H,Hu Z Q.Acta Metall Sin,2001;37:1233(刘金来,金涛,张静华,胡壮麒.金属学报,2001;37:1233) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|