| 等温锻造态TiAl基合金的超塑性研究 |
| 丁桦 潘志强 |
| 东北大学材料与冶金学院; 沈阳 110006 |
|
引用本文:
丁桦; 潘志强 . 等温锻造态TiAl基合金的超塑性研究[J]. 金属学报, 2000, 36(3): 304-307 .
[1] Cheng S C, Wolfenstine J, Sherby O D. Metall Trans, 1992;23A: 1509 [2] Imayev R M, Imayev V M, Salishev G A. J Mater Sci, 1992;27: 4465 [3] Lee W B, Yang H S, Kim Y W, Mukherjee A K. Scr MetallMater, 1993; 29: 1403 [4] Wajata T, Isonish K, Ameyama K, Tokizane M. ISIJ Int,1993; 33: 884 [5] Lee W B, Yang H S, Mukherjee A K. Mater Sci Eng, 1995;A192/193: 733 [6] Vanderschuren D, Nobuki M, Nakamura M. Scr MetallMater, 1993; 28: 605 [7] Nieh J G, Wadsworth J. Mater Sci Eng, 1997; A239/240: 88 [8] Huang B Y, He Y H, Deng Z Y, Wang J N, Sun J. ActaMetall Sin, 1998; 34: 1173 (黄伯云,贺跃辉,邓忠勇,王健农,孙坚.金属学报,1998;34:1173 [9] Zhou K C, Huang B Y, Qu X H, Chen X Q. Rare MetalMater Eng, 1998; 27: 336 (周科朝,黄伯云.曲选辉,陈小群.稀有金属材料与工程,1998;27: 336) [10] Shi X H, Zhang D, Ge Y, Qin J N, Zhang G D. Moter SciEng, 1998; 16: 24 (施幸华,张获,葛云,覃继宁,张国定.材料科学与工程,1998;16:24) [11] Zhang D, Qin J N, Shi X H, Zhang G D. Rare Metal MaterEng, 1998; 27: 210 (张获,覃继宁,施幸华,张国定.稀有金属材料与工程,1998;27: 210) [12] Yamaguchi M, Umakoshi Y eds., Ding S S trans. Intmetallica. Beijing: Sciences press, 1999: 40 (山口正治,马越佑吉著,丁树深译.金属间化合物.北京:科学出版社,1991:40) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|